Liaison Center for Innovative Dentistry, Graduate School of Dentistry, Tohoku University, Sendai, Japan.
Gerodontology. 2012 Dec;29(4):284-91. doi: 10.1111/j.1741-2358.2012.00639.x. Epub 2012 Jun 14.
Dynamic viscoelasticity is one of the most important characteristics of tissue conditioners. Leaching of plasticizer from tissue conditioners may cause changes in the dynamic viscoelasticity of these materials. The purpose of this study was to determine the dynamic viscoelasticity and plasticizer leachability of commercial tissue conditioners.
Five commercial tissue conditioners were used in this study: COE Comfort (CC), Fit Softer (FS), Hydro-Cast (HC), Soft Conditioner (SC) and Visco-Gel (VG). Five specimens of each material were stored in 37°C distilled water. The dynamic viscoelasticity and plasticizer leaching of each specimen were measured at 0, 1, 3, 7 and 14 days after immersion using a dynamic mechanical analyzer and high performance liquid chromatography. Data were analyzed using one-way anova and Student-Newman-Keuls test (α = 0.05).
Significant differences in dynamic viscoelasticity and plasticizer leaching were found among the materials. The dynamic viscoelasticity of all materials increased or decreased significantly with time. Rapid changes in dynamic viscoelasticity were evident on day 1 after water immersion. The material CC recorded the highest level of plasticizer leaching.
These results suggest that the dynamic viscoelasticity of commercial tissue conditioners is affected by plasticizer leaching. However, these effects are limited.
动态粘弹性是组织调理剂的最重要特性之一。从组织调理剂中浸出的增塑剂可能会导致这些材料的动态粘弹性发生变化。本研究的目的是确定商业组织调理剂的动态粘弹性和增塑剂浸出率。
本研究使用了 5 种商业组织调理剂:COE Comfort(CC)、Fit Softer(FS)、Hydro-Cast(HC)、Soft Conditioner(SC)和 Visco-Gel(VG)。每种材料的 5 个样本均储存在 37°C 的蒸馏水中。在浸泡 0、1、3、7 和 14 天后,使用动态机械分析仪和高效液相色谱法测量每个样本的动态粘弹性和增塑剂浸出率。使用单因素方差分析和 Student-Newman-Keuls 检验(α=0.05)对数据进行分析。
发现材料之间的动态粘弹性和增塑剂浸出率存在显著差异。所有材料的动态粘弹性随时间显著增加或减少。在水浸泡后的第 1 天,动态粘弹性的快速变化明显。CC 材料记录的增塑剂浸出水平最高。
这些结果表明,商业组织调理剂的动态粘弹性受增塑剂浸出的影响。然而,这些影响是有限的。