Root canal fillings are intended to prevent microbial proliferation over time in the canal after treatment. The objective of this study was to assess biofilm proliferation within the sealer-dentin interfaces of 2 methacrylate resin-based systems, self-etch (SE) and total-etch (TE), and an epoxy resin-based sealer (EP), aged for up to 6 months.
Standardized specimens (n = 45) comprising the coronal 5 mm of human roots were filled with the test materials and gutta-percha. Specimens were either not preincubated (control, n = 9) or were incubated in sterile saline for 1 week, 1 month, 3 months, or 6 months (n = 3/group). Monospecies biofilms of Enterococcus faecalis were grown on the specimens for 7 days in a chemostat-based biofilm fermentor mimicking pathogenic oral conditions. The extent of E. faecalis proliferation within the sealer-dentin interface for each material and incubation period group was assessed by using fluorescence microscopy of dihydroethidium-stained specimens.
TE had less biofilm proliferation than both EP and SE (P < .01). Deeper biofilm proliferation was detected in SE and EP specimens aged for 1 and 3 months than those aged for 1 week or 6 months (P < .05). Maximum depth of biofilm penetration was recorded for SE at 1 month (P < .05).
Within the test model used, the SE and EP sealers were more susceptible to interfacial biofilm proliferation than the TE restorative material. This susceptibility diminished after aging the materials' interfaces for 6 months.
根管填充旨在治疗后防止微生物在根管内随时间增殖。本研究的目的是评估 2 种甲基丙烯酸树脂基(自酸蚀 SE 和全酸蚀 TE)和 1 种环氧树脂基(EP)封闭剂在牙本质界面内的生物膜增殖情况,最长老化时间为 6 个月。
将包含人牙根冠部 5mm 的标准化样本(n=45)用测试材料和牙胶进行填充。样本要么不预孵育(对照组,n=9),要么在无菌盐水中孵育 1 周、1 个月、3 个月或 6 个月(n=3/组)。在类似于致病性口腔条件的基于化学恒化器的生物膜发酵器中,用粪肠球菌单种生物膜培养物在标本上生长 7 天,以评估每种材料和孵育期组中粪肠球菌在封闭剂-牙本质界面内的增殖程度。使用二氢乙啶染色标本的荧光显微镜评估各材料和孵育期组的粪肠球菌增殖程度。
TE 的生物膜增殖程度低于 EP 和 SE(P<.01)。与 1 周或 6 个月龄的标本相比,SE 和 EP 标本在 1 个月和 3 个月龄时检测到更深的生物膜增殖(P<.05)。SE 在 1 个月时记录到最大的生物膜穿透深度(P<.05)。
在所使用的测试模型中,SE 和 EP 封闭剂比 TE 修复材料更容易发生界面生物膜增殖。在将材料界面老化 6 个月后,这种易感性会降低。