Measurement of the mechanical properties of the ovine anterior cruciate ligament bone-ligament-bone complex: a basis for prosthetic evaluation.

作者信息

Rogers G J, Milthorpe B K, Muratore A, Schindhelm K

机构信息

Centre for Biomedical Engineering, University of New South Wales, Kensington, Australia.

出版信息

Biomaterials. 1990 Mar;11(2):89-96. doi: 10.1016/0142-9612(90)90122-7.

Abstract

The reported ultimate tensile stress of the anterior cruciate ligament varies greatly, ranging from 13 to 147 MPa. This study shows that the orientation and degree of flexion of the bone-ligament-bone complex significantly alter the apparent ultimate tensile properties (ultimate tensile stress ranging from 60 +/- 3 to 123 +/- 15 MPa, ultimate specific extension from 37 +/- 7 to 93 +/- 20%), whilst the method chosen for measuring extension also affects the calculated specific extension of the bone-ligament-bone complex. It is suggested that, for considerations of prosthesis design and evaluation, the mechanical properties of the bone-ligament-bone complex should be measured in anterior draw and extension measured using points as close as possible to the positions of the ligamentous attachment sites.

摘要

据报道,前交叉韧带的极限拉伸应力差异很大,范围在13至147兆帕之间。本研究表明,骨-韧带-骨复合体的取向和屈曲程度会显著改变其表观极限拉伸性能(极限拉伸应力范围为60±3至123±15兆帕,极限比伸长率为37±7至93±20%),而用于测量伸长的方法也会影响骨-韧带-骨复合体计算得出的比伸长率。建议在考虑假体设计和评估时,应在尽可能靠近韧带附着部位的位置使用前向牵拉和伸展测量来测定骨-韧带-骨复合体的力学性能。