Suppr超能文献

锡纸替代品污染对树脂义齿牙齿与义齿基托之间粘结强度影响的研究:一项体外研究。

An investigation on the influence of tin foil substitute contamination on bond strength between resin denture teeth and the denture base: an in vitro study.

作者信息

Bhaskaran Sapna, Hallikerimath R B

机构信息

Department of Prosthodontics, Noorul Islam College of Dental Sciences, Thiruvanthapuram, Kerala, India.

出版信息

Indian J Dent Res. 2012 Jul-Aug;23(4):556. doi: 10.4103/0970-9290.104975.

Abstract

STATEMENT OF PROBLEM

The problem of acrylic resin denture teeth separating from their denture base remains a major problem in prosthodontic practice and is frustrating to the patients as well as the dentists.

PURPOSE

This study investigated the influence of tin foil substitute contamination on bond strength between acrylic resin denture teeth and their denture base.

MATERIALS AND METHODS

A total of 80 modified acrylic resin maxillary left central incisors were processed to their denture base material. The 80 specimens were divided into two groups of 40 specimens each: the experimental group and the control group. The experimental group had the denture tooth ridge lap area contaminated with tin foil substitute.The 40 specimens in the control group were not contaminated. After 7 days of storage at room temperature, the bond strengths of the two groups were tested with a universal testing machine.The nature of failure was noted as adhesive (interface) or cohesive (in tooth or denture base material). The Welch test and z-test were performed to identify significant differences.

RESULTS

The uncontaminated specimens (group I) showed superior bond strength as compared to the contaminated specimens (group II); the difference in bond strength between the groups was highly significant (P<0.0001). Also the contaminated specimens exhibited predominantly adhesive failure (89.74%), whereas the uncontaminated specimens exhibited 55% adhesive failure and 45% cohesive failure.

CONCLUSION

Tin foil substitute contamination of the ridge laps of acrylic resin denture teeth greatly reduced the bond strength.

摘要

问题陈述

丙烯酸树脂假牙牙齿与其假牙基托分离的问题在口腔修复实践中仍然是一个主要问题,这让患者和牙医都感到沮丧。

目的

本研究调查了锡纸替代品污染对丙烯酸树脂假牙牙齿与其假牙基托之间粘结强度的影响。

材料与方法

共制作80颗改良的丙烯酸树脂上颌左中切牙作为假牙基托材料。80个样本分为两组,每组40个样本:实验组和对照组。实验组的假牙牙嵴搭接区域被锡纸替代品污染。对照组的40个样本未被污染。在室温下储存7天后,用万能试验机测试两组的粘结强度。记录失败的性质为粘结性(界面)或内聚性(在牙齿或假牙基托材料中)。进行韦尔奇检验和z检验以确定显著差异。

结果

未受污染的样本(第一组)与受污染的样本(第二组)相比,显示出更高的粘结强度;两组之间的粘结强度差异非常显著(P<0.0001)。此外,受污染的样本主要表现为粘结性失败(89.74%),而未受污染的样本粘结性失败率为55%,内聚性失败率为45%。

结论

丙烯酸树脂假牙牙齿的牙嵴搭接区域被锡纸替代品污染会大大降低粘结强度。