Carbohydr Polym. 2013 Feb 15;92(2):1705-10. doi: 10.1016/j.carbpol.2012.11.024. Epub 2012 Nov 17.
Tartaric acid (TA), a dicarboxylic acid, can act as a compatibiliser in starch/polyester blends. A mixture design was proposed to evaluate the effect of TA on the properties of starch/poly (butylene adipate co-terephthalate) (PBAT) blown films plasticised with glycerol. The interaction between the starch/PBAT and the TA has a positive effect on the tensile strength and puncture force. Additionally, greater proportions of TA increased Young's modulus. The starch+PBAT/TA and Gly/TA interactions contributed to a reduction in the water vapour permeability of the films. The inclusion of TA did not change the crystallinity of the samples. Formulations with intermediate proportions of TA (0.8 g/100 g) were shown to produce the best compatibilising effect. This was observed by DMA analysis as a consequence of the perfect equilibrium between the contributions of TA as a compatibiliser and in the acidolysis of starch, resulting in films with a tensile strength of 5.93 MPa, a possible alternative to non-biodegradable packaging.
酒石酸(TA)是一种二羧酸,可作为淀粉/聚酯共混物的增容剂。本文采用混合设计来评估 TA 对甘油增塑的淀粉/聚对苯二甲酸丁二醇酯(PBAT)吹塑薄膜性能的影响。淀粉/PBAT 与 TA 之间的相互作用对拉伸强度和穿刺力有积极影响。此外,TA 的比例越大,杨氏模量越高。淀粉+PBAT/TA 和 Gly/TA 相互作用有助于降低薄膜的水蒸气透过率。TA 的加入并没有改变样品的结晶度。含有中等比例 TA(0.8 g/100 g)的配方表现出最佳的增容效果。这可以通过 DMA 分析观察到,这是由于 TA 作为增容剂和淀粉酸解的贡献之间达到完美平衡的结果,得到的薄膜拉伸强度为 5.93 MPa,是一种可替代不可生物降解包装的材料。