This study evaluated the influence of chlorhexidine (CHX) on the microtensile bonds strength (µTBS) of resin core with two adhesive systems to dentin in endodontic cavities.
Flat dentinal surfaces in 40 molar endodontic cavities were treated with self-etch adhesive system, Contax (DMG) and total-etch adhesive system, Adper Single Bond 2 (3M ESPE) after the following surface treatments: (1) Priming only (Contax), (2) CHX for 15 sec + rinsing + priming (Contax), (3) Etching with priming (Adper Single Bond 2), (4) Etching + CHX for 15 sec + rinsing + priming (Adper Single Bond 2). Resin composite build-ups were made with LuxaCore (DMG) using a bulk method and polymerized for 40 sec. For each condition, half of specimens were submitted to µTBS after 24 hr storage and half of them were submitted to thermocycling of 10,000 cycles between 5℃ and 55℃ before testing. The data were analyzed using ANOVA and independent t-test at a significance level of 95%.
CHX pre-treatment did not affect the bond strength of specimens tested at the immediate testing period, regardless of dentin surface treatments. However, after 10,000 thermocycling, all groups showed reduced bond strength. The amount of reduction was greater in groups without CHX treatments than groups with CHX treatment. These characteristics were the same in both self-etch adhesive system and total-etch adhesive system.
2% CHX application for 15 sec proved to alleviate the decrease of bond strength of dentin bonding systems. No significant difference was shown in µTBS between total-etching system and self-etching system.
本研究评估洗必泰(CHX)对两种粘结系统粘结树脂核与根管治疗后牙本质微拉伸粘结强度(µTBS)的影响。
40颗磨牙根管治疗后的平坦牙本质表面,经以下表面处理后,分别用自酸蚀粘结系统Contax(DMG)和全酸蚀粘结系统Adper Single Bond 2(3M ESPE)处理:(1)仅涂底漆(Contax);(2)CHX处理15秒+冲洗+涂底漆(Contax);(3)酸蚀并涂底漆(Adper Single Bond 2);(4)酸蚀+CHX处理15秒+冲洗+涂底漆(Adper Single Bond 2)。使用LuxaCore(DMG)采用整块法制作树脂复合体桩核,聚合40秒。对于每种情况,一半的标本在储存24小时后进行µTBS测试,另一半在测试前进行5℃至55℃之间10000次循环的热循环。数据采用方差分析和独立t检验进行分析,显著性水平为95%。
无论牙本质表面处理如何,CHX预处理在即时测试期对测试标本粘结强度无影响。然而,在10000次热循环后,所有组的粘结强度均降低。未进行CHX处理的组粘结强度降低幅度大于进行CHX处理的组。自酸蚀粘结系统和全酸蚀粘结系统的这些特征相同。
2% CHX处理15秒可减轻牙本质粘结系统粘结强度的降低。全酸蚀系统和自酸蚀系统在µTBS方面无显著差异。