Suppr超能文献

牙龈沟液中白细胞介素-8 和白细胞介素-6 在镍铬合金烤瓷冠修复过程中的浓度变化。

The concentrations of IL-8 and IL-6 in gingival crevicular fluid during nickel-chromium alloy porcelain crown restoration.

机构信息

Department of Stomatology, The Sixth Affiliated People's Hospital of Shanghai Jiaotong University, No. 600 Yi Shan Road, Shanghai, 200233, China.

出版信息

J Mater Sci Mater Med. 2013 Jul;24(7):1717-22. doi: 10.1007/s10856-013-4924-3. Epub 2013 Apr 7.

Abstract

We explored gum irritation and cytotoxicity caused by nickel-chromium (Ni-Cr) alloy porcelain by interleukin-8 (IL-8), interleukin-6 (IL-6) and gingival crevicular fluid (GCF) volumes at different time points peri-crown restoration. This prospective study was conducted in 60 young adults. The total amount and concentrations of IL-8 and IL-6 per site, GCF volumes, and blood neutrophil counts were performed prior to and at 1 week, 3 months, and 6 months after Ni-Cr alloy-porcelain crown restoration. Thirty male and 30 female subjects, aged 20-35 years old were enrolled. The total amount and concentrations of IL-8 and IL-6 per site, GCF volumes increased after nickel-chromium (Ni-Cr) alloy-porcelain crown restoration, and reached its peak at the third month as the GCF volume increased by 52.20 %, the total amount and concentrations of IL-8 increased by 112.11 and 22.75 %; the total amount and concentrations of IL-6 increased by 77.66 and 17.17 % when compared to baseline. In particular, the increase of IL-8 concentration was found in female patients at 3 months after restoration; while the neutrophil count of the peripheral blood did not change significantly. The increase in the total amount and the concentrations of IL-8 and IL-6 and GCF volume may be related to the cytotoxicity induced by Ni-Cr alloy. The significant increase of IL-8 concentration in females indicates that more attention should be given to women during Ni-Cr alloy porcelain crown restoration.

摘要

我们通过白细胞介素-8(IL-8)、白细胞介素-6(IL-6)和牙龈沟液(GCF)体积在不同时间点的检测,探讨了镍铬(Ni-Cr)合金烤瓷对牙龈刺激和细胞毒性的影响。本前瞻性研究纳入了 60 名年轻成年人。在镍铬合金烤瓷冠修复前和修复后 1 周、3 个月和 6 个月,分别检测每个位点的 IL-8 和 IL-6 的总量和浓度、GCF 体积和外周血中性粒细胞计数。共纳入 30 名男性和 30 名女性受试者,年龄 20-35 岁。镍铬合金烤瓷冠修复后,每个位点的 IL-8 和 IL-6 总量和浓度、GCF 体积均增加,第 3 个月时 GCF 体积增加 52.20%,IL-8 总量和浓度增加 112.11%和 22.75%;IL-6 总量和浓度增加 77.66%和 17.17%,与基线相比。特别是在修复后 3 个月时,女性患者的 IL-8 浓度增加;而外周血中性粒细胞计数无明显变化。IL-8、IL-6 总量和浓度及 GCF 体积的增加可能与 Ni-Cr 合金的细胞毒性有关。女性 IL-8 浓度的显著增加表明,在进行 Ni-Cr 合金烤瓷冠修复时应更加关注女性。