Color stability of five orthodontic clear elastic ligatures.

作者信息

Soldati Dener C, Silva Roberta C, Oliveira Adauê S, Kaizer Marina R, Moraes Rafael R

机构信息

School of Dentistry, Federal University of Pelotas, RS, Brazil.

出版信息

Orthodontics (Chic.). 2013;14(1):e60-5. doi: 10.11607/ortho.892.

Abstract

AIM

In this study the color stability of five commercially available orthodontic clear elastic ligatures daily exposed to a staining agent (red wine) was investigated.

METHODS

The commercial brands tested were 3M Unitek, Abzil, American Orthodontics, Dentsply GAC, and Morelli. Baseline color readings (Commission Internationale de l'Eclairage [CIE] Lab* parameters) of 20 ligatures for each brand were carried out using a spectrophotometer. The ligatures were divided in two groups (n = 10): one group remained immersed in distilled water (control) throughout the period, while the other group was daily exposed to red wine (1 hour of immersion). Immersion media were daily renewed. Successive color readings were carried out after 7, 14, 21, and 28 days, and the chromatic variations calculated. Color variation data were analyzed by two-way repeated measures analysis of variance and Student-Newman-Keuls test (P < .05).

RESULTS

Storage in water increased staining until 14 days, and color receded after this period, irrespective of the brand. After 28 days of immersion in water, no significant difference among the commercial brands was observed. For the groups exposed to red wine, a significant increase in staining over the course of time was detected, irrespective of the brand. Ligatures from GAC and Morelli showed higher staining than the other materials, irrespective of the evaluation time. Ligatures from 3M Unitek and American generally showed lower pigmentation than the other brands.

CONCLUSION

Exposure to a staining agent, cumulative exposure time, and commercial brand are factors that influence the color stability of clear elastic ligatures.

摘要

目的

本研究调查了五种市售正畸透明弹性结扎圈每日暴露于染色剂(红酒)后的颜色稳定性。

方法

测试的商业品牌有3M Unitek、Abzil、American Orthodontics、Dentsply GAC和Morelli。使用分光光度计对每个品牌的20个结扎圈进行基线颜色读数(国际照明委员会[CIE]Lab*参数)。结扎圈分为两组(n = 10):一组在整个期间一直浸泡在蒸馏水中(对照组),而另一组每日暴露于红酒中(浸泡1小时)。浸泡介质每日更换。在第7、14、21和28天后进行连续颜色读数,并计算颜色变化。颜色变化数据通过双向重复测量方差分析和Student-Newman-Keuls检验进行分析(P <.05)。

结果

无论品牌如何,在水中储存会增加染色直至14天,此后颜色消退。在水中浸泡28天后,各商业品牌之间未观察到显著差异。对于暴露于红酒的组,无论品牌如何,在整个时间段内均检测到染色显著增加。无论评估时间如何,GAC和Morelli的结扎圈比其他材料显示出更高的染色。3M Unitek和American的结扎圈通常比其他品牌显示出更低的色素沉着。

结论

暴露于染色剂、累积暴露时间和商业品牌是影响透明弹性结扎圈颜色稳定性的因素。