Suppr超能文献

一项关于使用两种粘结系统(传统粘结剂和自酸蚀底漆(SEP))粘结正畸托槽失败率的对比临床研究。

A comparative clinical study of the failure rate of orthodontic brackets bonded with two adhesive systems: conventional and self-etching primer (SEP).

作者信息

Dominguez Gladys Cristina, Tortamano André, Lopes Luiz Vicente de Moura, Catharino Priscilla Campanatti Chibebe, Morea Camillo

机构信息

Department of Orthodontics and Pediatric Dentistry, School of Dentistry, São Paulo University (FOUSP), São Paulo, Brazil.

出版信息

Dental Press J Orthod. 2013 Mar-Apr;18(2):55-60. doi: 10.1590/s2176-94512013000200014.

Abstract

OBJECTIVE

This study compared the clinical performance of orthodontic brackets bonded with Transbond adhesive paste after two primer systems: a two-stage conventional system (acid etching + Transbond XT adhesive primer) and a single-stage self-etching primer (SEP) (Transbond Plus).

METHODS

The sample comprised 480 metal brackets bonded to the teeth of 24 consecutive patients treated for 36 to 48 months. A split-mouth design was used for bonding, and both systems were used in each patient. Bracket failure rates for each system were analyzed; and failure causes as reported by the patients and the quadrant of teeth for which brackets failed were recorded.

RESULTS

The conventional system group had a failure rate of 5.41%, whereas the rate for SEP was 4.58%. In this group, there were 5 failures (38.4%) in the right maxillary quadrant, 2 (15.4%) in the left maxillary quadrant, 4 (30.8%) in the right mandibular quadrant, and 2 (15.4%) in the left mandibular quadrant. In the SEP group, there were 4 (36.4%) failures in the right maxillary quadrant, 1 (9%) in the left maxillary quadrant, 3 (27.3%) in the right mandibular quadrant, and 3 (27.3%) in the left mandibular quadrant. Results of descriptive statistical analysis and odds ratio did not show any significant differences between rates (p = 0.67).

CONCLUSIONS

The clinical efficiency of SEP was similar to that of the conventional system.

摘要

目的

本研究比较了在两种底漆系统之后使用Transbond粘结剂粘贴正畸托槽的临床性能:两阶段传统系统(酸蚀+Transbond XT粘结剂底漆)和单阶段自酸蚀底漆(SEP)(Transbond Plus)。

方法

样本包括粘结在24例连续患者牙齿上的480个金属托槽,治疗时间为36至48个月。采用分口设计进行粘结,每位患者均使用两种系统。分析每个系统的托槽失败率;记录患者报告的失败原因以及托槽失败所在牙齿的象限。

结果

传统系统组的失败率为5.41%,而SEP组为4.58%。在该组中,右上颌象限有5例失败(38.4%),左上颌象限有2例(15.4%),右下颌象限有4例(30.8%),左下颌象限有2例(15.4%)。在SEP组中,右上颌象限有4例(36.4%)失败,左上颌象限有1例(9%),右下颌象限有3例(27.3%),左下颌象限有3例(27.3%)。描述性统计分析结果和优势比未显示两组失败率之间有任何显著差异(p = 0.67)。

结论

SEP的临床效率与传统系统相似。