Suppr超能文献

通过铒钇铝石榴石激光和车针进行牙体预备对牙本质黏结剂微渗漏的评估

Assessment of Tooth Preparation via Er:YAG Laser and Bur on Microleakage of Dentin Adhesives.

作者信息

Bahrololoomi Zahra, Heydari Elham

机构信息

Associate Professor, Department of Pediatric dentistry, Faculty of Dentistry, Shahid Sadoughi University of Medical Sciences, Yazd, Iran.

Dentist.

出版信息

J Dent (Tehran). 2014 Mar;11(2):172-8. Epub 2014 Mar 31.

Abstract

OBJECTIVE

Microleakage can be responsible for tooth hypersensitivity, secondary caries, and the possibility of pathological pulp alterations in restored teeth. Recently, alternative methods for tooth preparation such as laser irradiation have been studied; but there are limited studies on primary teeth. The aim of this in vitro study was to compare the degree of microleakage of composite restorations prepared by Er:YAG laser and conventional bur preparation with two adhesive systems in primary teeth.

MATERIALS AND METHODS

Eighty primary canine teeth were randomly divided into 4 groups. Class V cavities were prepared by Er:YAG laser or diamond bur on buccal surface. The groups were as follows: group1: High speed drill + self-etching adhesive Adper Prompt-L-Pop, group 2: Er:YAG laser + etch & rinse adhesive Adper Single Bond, group 3: High speed drill + Adper Single Bond, group 4: Er:YAG laser + Adper Prompt-L-Pop. Cavities were restored with Filtek Z250 composite resin. Then all of the specimens were polished, thermocycled, immersed in 2% methylene blue solution and sectioned longitudinally. Degree of microleakage was evaluated by two evaluators who assigned the micrleakage score (0 to 3). The original data were analyzed by the Kruskal-Wallis and Dunn's tests.

RESULTS

There were significant differences between bur-prepared cavities in the Adper Single Bond and other groups. There were no statistically significant differences between other groups.

CONCLUSION

Laser-prepared cavities showed higher microleakage scores than cavities prepared with diamond bur with etch and rinse adhesive system. No significant difference was revealed between the laser and bur-prepared cavities using self-etch primers.

摘要

目的

微渗漏可导致牙齿过敏、继发龋以及修复牙发生牙髓病变的可能性。近来,诸如激光照射等备牙的替代方法已得到研究;但关于乳牙的研究有限。本体外研究的目的是比较在乳牙中使用两种粘结系统时,用铒激光和传统车针备牙后复合树脂修复体的微渗漏程度。

材料与方法

80颗乳尖牙随机分为4组。在颊面用铒激光或金刚砂车针制备Ⅴ类洞。分组如下:组1:高速车针+自酸蚀粘结剂Adper Prompt-L-Pop;组2:铒激光+酸蚀冲洗粘结剂Adper Single Bond;组3:高速车针+Adper Single Bond;组4:铒激光+Adper Prompt-L-Pop。用Filtek Z250复合树脂修复窝洞。然后所有标本进行抛光、热循环处理,浸入2%亚甲蓝溶液中并纵向切片。由两名评估者评估微渗漏程度并给出微渗漏评分(0至3分)。原始数据采用Kruskal-Wallis检验和Dunn检验进行分析。

结果

使用Adper Single Bond粘结剂的车针备洞组与其他组之间存在显著差异。其他组之间无统计学显著差异。

结论

激光备洞的微渗漏评分高于使用酸蚀冲洗粘结系统的金刚砂车针备洞。使用自酸蚀底漆时,激光备洞和车针备洞之间未显示出显著差异。