Insabralde Natalia Martins, Poletti Thaís, Conti Ana Cláudia, Oltramari-Navarro Paula Vanessa, Lopes Murilo B, Flores-Mir Carlos, de Almeida Marcio Rodrigues
Department of Orthodontics, University of North Parana, UNOPAR, Londrina, Paraná, Brazil.
Prog Orthod. 2014 May 30;15(1):42. doi: 10.1186/s40510-014-0042-0.
The objective of this study is to evaluate the force-deflection behavior of beta-titanium alloy wires between two leveled and unleveled bracket alignment scenarios using a three-point bending test.
Six groups of ten beta-titanium alloy wire segments (0.017 × 0.025-in. diameter) of different manufacturers (Orthometric, Ortho Organizers, GAC, Morelli, and Ormco) were used. Both brackets were bonded to an acrylic jig with a 10-mm interbracket distance. A 1-mm deflection test in two hypothetical conditions (with aligned brackets and by simulating a 2-mm horizontal displacement of the brackets) was explored. Forces of activation and deactivation of the wires during both tests were compared by an analysis of variance (ANOVA) tests followed by a Tukey test.
A statistically significant difference was found in the force-deflection behavior between some of the wires in both simulated in vitro conditions. For the leveled-type alignment scenario, the differences between wires were up to 70 g (range 110 to 179 g). For the unleveled-type alignment scenario, these differences were up to 65 g (range 111 to 175 g).
The study showed some significant differences in forces generated during activation and deactivation among the five types of beta-titanium wires tested. In comparing leveled and unleveled brackets during activation, only Orthometric Beta Flexy and Ormco Beta-titanium were different between them.
本研究的目的是通过三点弯曲试验评估在两种整平与未整平托槽排列情况下β钛合金丝的力-挠度行为。
使用了六组每组十段不同制造商(Orthometric、Ortho Organizers、GAC、Morelli和Ormco)的β钛合金丝(直径0.017×0.025英寸)。两个托槽均粘结到一个丙烯酸夹具上,托槽间距离为10毫米。探索了在两种假设条件下(托槽对齐和模拟托槽2毫米水平位移)的1毫米挠度试验。通过方差分析(ANOVA)试验及随后的Tukey检验比较了两种试验过程中丝的激活和去激活力。
在两种模拟体外条件下,部分丝之间的力-挠度行为存在统计学显著差异。对于整平型排列情况,丝之间的差异高达70克(范围为110至179克)。对于未整平型排列情况,这些差异高达65克(范围为111至175克)。
该研究表明,在测试的五种β钛丝中,激活和去激活过程中产生的力存在一些显著差异。在激活过程中比较整平和未整平托槽时,只有Orthometric Beta Flexy和Ormco Beta - 钛两者之间存在差异。