Université du Havre, URCOM, EA 3221, FR CNRS 3038, 25, rue Philippe Lebon CS 80540, 76058 Le Havre Cedex, France.
Carbohydr Polym. 2014 Nov 4;112:334-41. doi: 10.1016/j.carbpol.2014.05.094. Epub 2014 Jun 8.
Filament stretchability of xanthan gum (XG) and hydroxypropyl guar (HPG) was investigated in aqueous solutions (0.125, 0.25, 0.5, 1, 1.2 and 1.5% w/w) and in O/W emulsions using a texture analyzer. Additionally, rheological characterizations were carried out on the systems and shear and oscillation parameters were used to interpret stretching properties. XG solutions exhibited a solid-like behavior with rheological parameters much higher than for HPG one whatever the concentration. Filament stretching values of XG solutions were superior to HPG for concentration below 1% w/w and then became comparable for higher concentrations. No meaningful relationship was found between rheological and stretching values. Synergy was observed for all XG/HPG mixtures at 0.125, 0.25 and 0.5% influencing both the rheological and the filament stretching values. The 25/75 XG/HPG ratio showed the maximum synergistic effect at all concentrations while the filament stretchability was enhanced in a wider range of ratios. XG and HPG did not present the same behavior in emulsions. No clear synergistic effect was observed and XG markedly influenced the emulsion filament stretching.
研究了黄原胶(XG)和羟丙基瓜尔胶(HPG)在水溶液(0.125、0.25、0.5、1、1.2 和 1.5%w/w)和 O/W 乳液中的长丝拉伸性能,使用质构分析仪进行。此外,还对体系进行了流变特性分析,并使用剪切和振荡参数来解释拉伸性能。无论浓度如何,XG 溶液的流变参数都明显高于 HPG,表现出固态行为。XG 溶液的长丝拉伸值在低于 1%w/w 的浓度下优于 HPG,然后在更高的浓度下变得相当。流变学和拉伸值之间没有发现有意义的关系。在所有 XG/HPG 混合物的浓度为 0.125、0.25 和 0.5%时,都观察到协同作用,影响流变学和长丝拉伸值。在所有浓度下,25/75XG/HPG 比例表现出最大的协同效应,而长丝拉伸性在更宽的比例范围内得到增强。XG 和 HPG 在乳液中的行为并不相同。没有观察到明显的协同效应,XG 显著影响乳液长丝拉伸性。