Filippidis George, Mari Meropi, Kelegkouri Lambrini, Philippidis Aggelos, Selimis Aleksandros, Melessanaki Kristallia, Sygletou Maria, Fotakis Costas
1Institute of Electronic Structure and Laser,Foundation for Research and Technology Hellas,PO Box 1527,Heraklion 71110,Crete,Greece.
Microsc Microanal. 2015 Apr;21(2):510-7. doi: 10.1017/S1431927614013580. Epub 2014 Nov 18.
The present work investigates the applicability of nonlinear imaging microscopy for the precise assessment of degradation of the outer protective layers of painted artworks as a function of depth due to aging. Two fresh and artificially aged triterpenoid varnishes, dammar and mastic, were tested. Nonlinear imaging techniques have been employed as a new diagnostic tool for determination of the exact thickness of the affected region due to artificial aging of the natural varnishes. The measured thicknesses differ from the calculated mean penetration depths of the samples. These nondestructive, high resolution modalities are valuable analytical tools for aging studies and they have the potential to provide unique in-depth information. Single photon laser induced fluorescence measurements and Raman spectroscopy were used for the integrated investigation and analysis of aging effects in varnishes.
本研究探讨了非线性成像显微镜在精确评估绘画艺术品外层保护层因老化而随深度变化的降解情况方面的适用性。测试了两种新鲜的和人工老化的三萜类清漆,达玛树脂和乳香脂。非线性成像技术已被用作一种新的诊断工具,用于确定天然清漆人工老化后受影响区域的精确厚度。测量的厚度与样品计算出的平均渗透深度不同。这些无损、高分辨率的模态是老化研究中有价值的分析工具,它们有潜力提供独特的深度信息。单光子激光诱导荧光测量和拉曼光谱被用于清漆老化效应的综合研究和分析。