Engstrand Johanna, Aberg Jonas, Engqvist Håkan
Applied Materials Science, Department of Engineering Sciences, Uppsala University, Sweden.
Mater Sci Eng C Mater Biol Appl. 2013 Jan 1;33(1):527-31. doi: 10.1016/j.msec.2012.09.026. Epub 2012 Oct 6.
Handling of calcium phosphate cements is difficult, where problems often arise during mixing, transferring to syringes, and subsequent injection. Via the use of premixed cements the risk of handling complications is reduced. However, for premixed cements to work in a clinical situation the setting time needs to be improved. The objective of this study is to investigate the influence of the addition of water on the properties of premixed cement. Monetite-forming premixed cements with small amounts of added water (less than 6.8 wt.%) were prepared and the influence on injectability, working time, setting time and mechanical strength was evaluated. The results showed that the addition of small amounts of water had significant influence on the properties of the premixed cement. With the addition of just 1.7 wt.% water, the force needed to extrude the cement from a syringe was reduced from 107 (±15) N to 39 (±9) N, the compression strength was almost doubled, and the setting time decreased from 29 (±4) min to 19 (±2) min, while the working time remained 5 to 6h. This study demonstrates the importance of controlling the water content in premixed cement pastes and how water can be used to improve the properties of premixed cements.
磷酸钙骨水泥的操作很困难,在混合、转移至注射器以及随后的注射过程中经常会出现问题。通过使用预混骨水泥,可降低操作并发症的风险。然而,为使预混骨水泥在临床情况下发挥作用,需要改进其凝固时间。本研究的目的是探讨加水对预混骨水泥性能的影响。制备了添加少量水(小于6.8重量%)的生成透钙磷石的预混骨水泥,并评估了其对可注射性、工作时间、凝固时间和机械强度的影响。结果表明,添加少量水对预混骨水泥的性能有显著影响。仅添加1.7重量%的水,将骨水泥从注射器中挤出所需的力就从107(±15)N降至39(±9)N,抗压强度几乎翻倍,凝固时间从29(±4)分钟降至19(±2)分钟,而工作时间保持在5至6小时。本研究证明了控制预混骨水泥浆体含水量的重要性以及水如何用于改善预混骨水泥的性能。