Fujihara Ami, Shimada Naohiko, Maruyama Atsushi, Ishihara Kazuhiko, Nakai Keita, Yusa Shin-ichi
Department of Materials Science and Chemistry, University of Hyogo, 2167 Shosha, Himeji, Hyogo 671-2280, Japan.
Soft Matter. 2015 Jul 14;11(26):5204-13. doi: 10.1039/c5sm00499c. Epub 2015 May 14.
Poly(2-ureidoethyl methacrylate) (PUEM) was prepared via reversible addition-fragmentation chain transfer (RAFT) controlled radical polymerization and a post-modification reaction. PUEM shows upper critical solution temperature (UCST) behavior in aqueous solution. Although PUEM can dissolve in water above the UCST, it cannot dissolve in water below the UCST. Diblock copolymers (MmUn) composed of a biocompatible hydrophilic poly(2-methacryloyloxyethyl phosphorylcholine) (PMPC) block and a PUEM block with different compositions were prepared via RAFT radical polymerization and a post-modification reaction. "M" and "U" represent PMPC and PUEM blocks, respectively, and the subscripts represent the degree of polymerization of each block. M95U149 and M20U163 formed polymer micelles comprising a PUEM core and a PMPC shell below the critical aggregation temperature (Tc) in aqueous solution. Polymer micelles were formed from M20U163 below 32 °C, which can incorporate guest molecules into the core.
聚(甲基丙烯酸2-脲基乙酯)(PUEM)通过可逆加成-断裂链转移(RAFT)可控自由基聚合和后修饰反应制备而成。PUEM在水溶液中表现出上临界溶液温度(UCST)行为。虽然PUEM在UCST以上能溶于水,但在UCST以下则不溶于水。通过RAFT自由基聚合和后修饰反应制备了由生物相容性亲水性聚(2-甲基丙烯酰氧基乙基磷酰胆碱)(PMPC)嵌段和不同组成的PUEM嵌段组成的二嵌段共聚物(MmUn)。“M”和“U”分别代表PMPC和PUEM嵌段,下标表示各嵌段的聚合度。M95U149和M20U163在水溶液中的临界聚集温度(Tc)以下形成了由PUEM核和PMPC壳组成的聚合物胶束。M20U163在32℃以下形成聚合物胶束,其可将客体分子纳入核中。