Suppr超能文献

热塑性和新型热固性弹性结扎带的力衰减和尺寸变化。

Force decay and dimensional changes of thermoplastic and novel thermoset elastomeric ligatures.

作者信息

Masoud Ahmed I, Bulic Milena, Viana Grace, Bedran-Russo Ana K

机构信息

a  Faculty member, Department of Orthodontics, Faculty of Dentistry, King Abdulaziz University, Jeddah, Saudi Arabia; and Clinical Assistant Professor, Department of Orthodontics, College of Dentistry, University of Illinois at Chicago, Chicago, IL.

b  Orthodontic Resident, Department of Orthodontics, College of Dentistry, University of Illinois at Chicago, Chicago, IL.

出版信息

Angle Orthod. 2016 Sep;86(5):818-25. doi: 10.2319/082815-581.1. Epub 2016 Jan 7.

Abstract

OBJECTIVES

To compare over a period of 8 weeks (1) the force decay and (2) the dimensional changes between thermoplastic (TP) and thermoset (TS) elastomeric ligatures.

MATERIALS AND METHODS

TP and TS elastomeric ligatures were obtained from Rocky Mountain Orthodontics™. The TS ligatures were custom made specifically for this study. The sample included 72 clear TP and 72 clear TS elastomeric ligatures. The experiment was performed in a simulated oral environment (pH of 6.75) at 37°C. The remaining forces and the dimensional changes were measured at different time points over a period of 8 weeks.

RESULTS

Student's t-tests revealed significant differences in percent force loss, percent change in outer diameter, percent change in inner diameter, and percent change in wall thickness between TP and TS elastomeric ligatures across all time points (P < .001). The difference in percent change in width between TP and TS elastomeric ligatures was not significant at all time points (P > .05). The mean difference in force loss between TP and TS across all time points was 22.91%. The TP and TS specimens exhibited 93.04% and 77.41% force loss, respectively, at the 28th day.

CONCLUSIONS

This novel TS elastomeric ligature showed significantly less force decay and dimensional changes over time; therefore, it might be superior during initial leveling and aligning and during finishing stages. Using a transfer jig to prevent relaxation of the specimens before force measurement showed that force decay of commercially available elastomeric ligatures was greater than that described in previous publications.

摘要

目的

在8周的时间内比较(1)热塑性(TP)和热固性(TS)弹性结扎丝之间的力衰减情况,以及(2)尺寸变化情况。

材料与方法

TP和TS弹性结扎丝购自落基山正畸公司(Rocky Mountain Orthodontics™)。TS结扎丝是专门为本研究定制的。样本包括72根透明TP弹性结扎丝和72根透明TS弹性结扎丝。实验在37°C、pH值为6.75的模拟口腔环境中进行。在8周的时间内,于不同时间点测量剩余力和尺寸变化。

结果

学生t检验显示,在所有时间点上,TP和TS弹性结扎丝在力损失百分比、外径变化百分比、内径变化百分比和壁厚变化百分比方面存在显著差异(P < .001)。TP和TS弹性结扎丝在宽度变化百分比上的差异在所有时间点均不显著(P > .05)。所有时间点上TP和TS之间的平均力损失差异为22.91%。在第28天时,TP和TS样本的力损失分别为93.04%和77.41%。

结论

这种新型TS弹性结扎丝随时间推移显示出显著更少的力衰减和尺寸变化;因此,在初始整平排齐阶段和精细调整阶段可能更具优势。在力测量前使用转移夹具防止样本松弛,结果显示市售弹性结扎丝的力衰减大于先前出版物中所述。

相似文献

3
Strength decay of orthodontic elastomeric ligatures.正畸弹性结扎丝的强度衰减
J Orthod. 2002 Mar;29(1):37-43. doi: 10.1093/ortho/29.1.37.
4
Force decay and deformation of orthodontic elastomeric ligatures.正畸弹性结扎圈的力衰减与变形
Am J Orthod Dentofacial Orthop. 1997 Jan;111(1):1-11. doi: 10.1016/s0889-5406(97)70295-6.
7
Discoloration and force degradation of orthodontic elastomeric ligatures.正畸弹性结扎丝的变色与力值衰减。
Dental Press J Orthod. 2017 Mar-Apr;22(2):45-54. doi: 10.1590/2177-6709.22.2.045-054.oar.

本文引用的文献

6
The wisdom of the bioprogressive philosophy.生物进步主义哲学的智慧。
Semin Orthod. 1998 Dec;4(4):201-9. doi: 10.1016/s1073-8746(98)80025-x.
7
Force degradation in elastomeric chains.
Semin Orthod. 1997 Sep;3(3):189-97. doi: 10.1016/s1073-8746(97)80069-2.
8
Force decay and deformation of orthodontic elastomeric ligatures.正畸弹性结扎圈的力衰减与变形
Am J Orthod Dentofacial Orthop. 1997 Jan;111(1):1-11. doi: 10.1016/s0889-5406(97)70295-6.
9
Force decay of elastomeric chain--a serial study. Part II.弹性链的力衰减——系列研究。第二部分。
Am J Orthod Dentofacial Orthop. 1993 Oct;104(4):373-7. doi: 10.1016/S0889-5406(05)81336-8.

文献检索

告别复杂PubMed语法,用中文像聊天一样搜索,搜遍4000万医学文献。AI智能推荐,让科研检索更轻松。

立即免费搜索

文件翻译

保留排版,准确专业,支持PDF/Word/PPT等文件格式,支持 12+语言互译。

免费翻译文档

深度研究

AI帮你快速写综述,25分钟生成高质量综述,智能提取关键信息,辅助科研写作。

立即免费体验