Gitt H A, Hlubna-Daum E, Zennig S
Stomatol DDR. 1977 Jul;27(7):395-9.
Four tissue adhesives of the butylcyano-acrylate type were tested for breaking strength. The addition of dyes and stabilizers results in an increase in breaking strength. Adhesives coloured with an anthraquinone dye and stabilized with SO2 significantly surpass in breaking strength adhesives that are only coloured or stabilized. Fiomed II (coloured, stabilized with SO2) yields significantly (at P=0.001) better values than Histoacryl blue. Addition of the dye alone seems to exert a better effect on breaking strength than addition of the stabilizer alone. As evidenced by our results, the breaking strength is in the order: 1. Fiomed II (coloured, stabilized with SO2), 2. Histoacryl blue, 3. Fiomed III (coloured, without SO2), 4. Fiomed I (without dye, stabilized with SO2).
对四种丁基氰基丙烯酸酯类组织粘合剂进行了抗断裂强度测试。添加染料和稳定剂会导致抗断裂强度增加。用蒽醌染料着色并用二氧化硫稳定的粘合剂在抗断裂强度上明显超过仅着色或仅稳定的粘合剂。Fiomed II(着色,用二氧化硫稳定)的抗断裂强度值(P = 0.001)明显优于Histoacryl blue。单独添加染料对抗断裂强度的影响似乎比单独添加稳定剂更好。我们的结果表明,抗断裂强度顺序为:1. Fiomed II(着色,用二氧化硫稳定),2. Histoacryl blue,3. Fiomed III(着色,无二氧化硫),4. Fiomed I(无染料,用二氧化硫稳定)。