Suppr超能文献

红葡萄酒和白葡萄酒对纳米填充和纳米混合树脂复合材料颜色变化的影响。

The effect of red and white wine on color changes of nanofilled and nanohybrid resin composites.

作者信息

Tanthanuch Saijai, Kukiattrakoon Boonlert, Peerasukprasert Thanwalee, Chanmanee Nilobon, Chaisomboonphun Parnchanok, Rodklai Apisara

机构信息

Department of Conservative Dentistry, Faculty of Dentistry, Prince of Songkla University, Hat Yai, Songkhla, Thailand.; Dental Materials Research Unit, Faculty of Dentistry, Prince of Songkla University, Hat Yai, Songkhla, Thailand.

Department of Conservative Dentistry, Faculty of Dentistry, Prince of Songkla University, Hat Yai, Songkhla, Thailand.

出版信息

Restor Dent Endod. 2016 May;41(2):130-6. doi: 10.5395/rde.2016.41.2.130. Epub 2016 May 3.

Abstract

OBJECTIVES

This study investigated the effect of red and white wine on color changes of nanofilled and nanohybrid resin composite.

MATERIALS AND METHODS

Sixty specimens of each resin composite were prepared. Baseline data color values were recorded using a spectrophotometer. Three groups of discs (n = 20) were then alternately immersed in red, white wine, and deionized water (as a control) for twenty five minutes and artificial saliva for five minutes for four cycles. Specimens were then stored in artificial saliva for twenty two hours. This process was repeated for five days following immersion in artificial saliva for two days. Subsequently, the process was repeated again. Data were analyzed by two-way repeated ANOVA, one-way ANOVA, and Tukey's HSD.

RESULTS

Red wine caused significantly higher color change (ΔE(*) > 3.3) than did white wine and deionized water (p < 0.05). Nanohybrid resin composites had significantly more color changes than nanofilled resin composite (p < 0.05).

CONCLUSIONS

The effect of red and white wine on the color changes of resin composite restorative materials depended upon the physical and chemical composition of the restorative materials and the types of wine.

摘要

目的

本研究调查了红葡萄酒和白葡萄酒对纳米填充和纳米混合树脂复合材料颜色变化的影响。

材料与方法

制备每种树脂复合材料的60个样本。使用分光光度计记录基线数据颜色值。然后将三组圆盘(n = 20)交替浸泡在红葡萄酒、白葡萄酒和去离子水中(作为对照)25分钟,再浸泡在人工唾液中5分钟,共进行四个循环。之后将样本在人工唾液中储存22小时。在浸泡于人工唾液两天后,此过程重复五天。随后,再次重复该过程。数据通过双向重复方差分析、单向方差分析和Tukey's HSD进行分析。

结果

红葡萄酒引起的颜色变化(ΔE(*) > 3.3)显著高于白葡萄酒和去离子水(p < 0.05)。纳米混合树脂复合材料的颜色变化显著多于纳米填充树脂复合材料(p < 0.05)。

结论

红葡萄酒和白葡萄酒对树脂复合材料修复材料颜色变化的影响取决于修复材料的物理和化学组成以及葡萄酒的类型。

相似文献

引用本文的文献

本文引用的文献

4
Update on dental nanocomposites.牙科纳米复合材料的最新进展。
J Dent Res. 2010 Jun;89(6):549-60. doi: 10.1177/0022034510363765. Epub 2010 Mar 18.
5
Color measurement in dentistry.牙科中的颜色测量。
J Dent. 2009;37 Suppl 1:e2-6. doi: 10.1016/j.jdent.2009.03.011. Epub 2009 Apr 29.
6
Color stability evaluation of aesthetic restorative materials.美学修复材料的颜色稳定性评估
Braz Oral Res. 2008 Jul-Sep;22(3):205-10. doi: 10.1590/s1806-83242008000300003.

文献检索

告别复杂PubMed语法,用中文像聊天一样搜索,搜遍4000万医学文献。AI智能推荐,让科研检索更轻松。

立即免费搜索

文件翻译

保留排版,准确专业,支持PDF/Word/PPT等文件格式,支持 12+语言互译。

免费翻译文档

深度研究

AI帮你快速写综述,25分钟生成高质量综述,智能提取关键信息,辅助科研写作。

立即免费体验