Suppr超能文献

取出后中心静脉端口导管的机械性能和表面特性:聚氨酯和硅橡胶材料的比较。

Mechanic and surface properties of central-venous port catheters after removal: A comparison of polyurethane and silicon rubber materials.

作者信息

Braun Ulrike, Lorenz Edelgard, Weimann Christiane, Sturm Heinz, Karimov Ilham, Ettl Johannes, Meier Reinhard, Wohlgemuth Walter A, Berger Hermann, Wildgruber Moritz

机构信息

BAM Federal Institute for Materials Research and Testing, Unter den Eichen 87, 12200 Berlin, Germany.

BAM Federal Institute for Materials Research and Testing, Unter den Eichen 87, 12200 Berlin, Germany.

出版信息

J Mech Behav Biomed Mater. 2016 Dec;64:281-91. doi: 10.1016/j.jmbbm.2016.08.002. Epub 2016 Aug 5.

Abstract

Central venous port devices made of two different polymeric materials, thermoplastic polyurethane (TPU) and silicone rubber (SiR), were compared due their material properties. Both naïve catheters as well as catheters after removal from patients were investigated. In lab experiments the influence of various chemo-therapeutic solutions on material properties was investigated, whereas the samples after removal were compared according to the implanted time in patient. The macroscopic, mechanical performance was assessed with dynamic, specially adapted tests for elasticity. The degradation status of the materials was determined with common tools of polymer characterisation, such as infrared spectroscopy, molecular weight measurements and various methods of thermal analysis. The surface morphology was analysed using scanning electron microscopy. A correlation between material properties and clinical performance was proposed. The surface morphology and chemical composition of the polyurethane catheter materials can potentially result in increased susceptibility of the catheter to bloodstream infections and thrombotic complications. The higher mechanic failure, especially with increasing implantation time of the silicone catheters is related to the lower mechanical performance compared to the polyurethane material as well as loss of barium sulphate filler particles near the surface of the catheter. This results in preformed microscopic notches, which act as predetermined sites of fracture.

摘要

对由两种不同聚合材料——热塑性聚氨酯(TPU)和硅橡胶(SiR)制成的中心静脉端口装置进行了材料性能比较。研究了未使用过的导管以及从患者体内取出后的导管。在实验室实验中,研究了各种化疗溶液对材料性能的影响,而对取出后的样本则根据其在患者体内的植入时间进行比较。通过动态的、专门适配的弹性测试来评估宏观机械性能。使用聚合物表征的常用工具,如红外光谱、分子量测量和各种热分析方法来确定材料的降解状态。使用扫描电子显微镜分析表面形态。提出了材料性能与临床性能之间的相关性。聚氨酯导管材料的表面形态和化学成分可能会导致导管对血流感染和血栓形成并发症的易感性增加。硅橡胶导管较高的机械故障,尤其是随着植入时间的增加,与聚氨酯材料相比机械性能较低以及导管表面附近硫酸钡填充颗粒的损失有关。这会形成预先存在的微观缺口,这些缺口成为预定的断裂部位。