Nisula Mikko, Linnera Jarno, Karttunen Antti J, Karppinen Maarit
Department of Chemistry and Materials Science, Aalto University, 00076, Aalto, Finland.
Chemistry. 2017 Mar 2;23(13):2988-2992. doi: 10.1002/chem.201605816. Epub 2017 Jan 31.
Crystalline Li-organic thin films are grown with the atomic/molecular layer deposition (ALD/MLD) technique from lithium hexamethyldisilazide and hydroquinone. The as-deposited films are found to undergo a reversible structural transformation upon exposure to ambient humid air. According to density functional theory calculations, the guest-induced transformation may be related to an unsaturated Li site in the crystal structure.