Porwal Anand, Khandelwal Meenakshi, Punia Vikas, Sharma Vivek
Department of Prosthodontics and Crown and Bridge, Darshan Dental College and Hospital, Udaipur, Rajasthan, India.
J Indian Prosthodont Soc. 2017 Jan-Mar;17(1):61-67. doi: 10.4103/0972-4052.197940.
The purpose of this study was to evaluate the effect of different denture cleansers on the color stability, surface hardness, and roughness of different denture base resins.
Three denture base resin materials (conventional heat cure resin, high impact resin, and polyamide denture base resin) were immersed for 180 days in commercially available two denture cleansers (sodium perborate and sodium hypochlorite). Color, surface roughness, and hardness were measured for each sample before and after immersion procedure.
One-way analysis of variance and Tukey's honestly significant difference test were used to evaluate color, surface roughness, and hardness data before and after immersion in denture cleanser (α =0.05).
All denture base resins tested exhibited a change in color, surface roughness, and hardness to some degree in both denture cleansers. Polyamides resin immersed in sodium perborate showed a maximum change in color after immersion for 180 days. Conventional heat cure resin immersed in sodium hypochlorite showed a maximum change in surface roughness and conventional heat cure immersed in sodium perborate showed a maximum change in hardness.
Color changes of all denture base resins were within the clinically accepted range for color difference. Surface roughness change of conventional heat cure resin was not within the clinically accepted range of surface roughness. The choice of denture cleanser for different denture base resins should be based on the chemistry of resin and cleanser, denture cleanser concentration, and duration of immersion.
本研究的目的是评估不同义齿清洁剂对不同义齿基托树脂的颜色稳定性、表面硬度和粗糙度的影响。
将三种义齿基托树脂材料(传统热固化树脂、高抗冲树脂和聚酰胺义齿基托树脂)在市售的两种义齿清洁剂(过硼酸钠和次氯酸钠)中浸泡180天。在浸泡前后对每个样品进行颜色、表面粗糙度和硬度测量。
采用单因素方差分析和Tukey真实显著性差异检验来评估浸泡在义齿清洁剂前后的颜色、表面粗糙度和硬度数据(α =0.05)。
所有测试的义齿基托树脂在两种义齿清洁剂中均在一定程度上表现出颜色、表面粗糙度和硬度的变化。浸泡在过硼酸钠中的聚酰胺树脂在浸泡180天后颜色变化最大。浸泡在次氯酸钠中的传统热固化树脂表面粗糙度变化最大,浸泡在过硼酸钠中的传统热固化树脂硬度变化最大。
所有义齿基托树脂的颜色变化均在临床可接受的色差范围内。传统热固化树脂的表面粗糙度变化不在临床可接受的表面粗糙度范围内。针对不同义齿基托树脂选择义齿清洁剂应基于树脂和清洁剂的化学性质、义齿清洁剂浓度以及浸泡时间。