[牙科自凝树脂的研究。(17)。聚甲基丙烯酸甲酯与牛牙釉质或牙科合金的黏附性(作者译)]

[Studies on dental self-curing resins. (17). Adhesion of PMMA with bovine enamel or dental alloys (author's transl)].

作者信息

Takeyama M, Kashibuchi S, Nakabayashi N, Masuhara E

出版信息

Shika Rikogaku Zasshi. 1978 Jul;19(47):179-85.

PMID:282386
Abstract

We synthesized 4-methacryloxyethyl trimellite acid (4-MET) and anhydride (4-META), and tried them as a reactive comonomer for adhesives to bovine enamel. In the case of non-etched enamel, tensile adhesive strength was 40-50 Kg/cm2 after one day immersion in 37 degrees C water, but it decreased below 10 Kg/cm2 after a month immersion in 37 degrees C water. It could be concluded that this adhesion was not sufficient for practical usage. Then we applied this method to an etched enamel. After a series of experiments we concluded that it was necessary to etch bovine enamel surface with 30% citric acid for practical usage. Adhesion of some dental alloys with a PMMA rod was also studied and adhesive strength in Co-Cr alloy was over 150 Kg/cm2 either after one month immersion in 37 degrees C water or 60 times thermal cycles between 4 degrees C and 60 degrees C.

摘要

我们合成了4-甲基丙烯酰氧乙基偏苯三酸(4-MET)及其酸酐(4-META),并将它们作为用于牛牙釉质的粘合剂的反应性共聚单体进行试验。对于未蚀刻的牙釉质,在37℃水中浸泡一天后,拉伸粘结强度为40-50 Kg/cm2,但在37℃水中浸泡一个月后,其粘结强度降至10 Kg/cm2以下。可以得出结论,这种粘结力对于实际应用来说是不够的。然后我们将此方法应用于蚀刻后的牙釉质。经过一系列实验后,我们得出结论,为了实际应用,有必要用30%的柠檬酸蚀刻牛牙釉质表面。我们还研究了一些牙科合金与聚甲基丙烯酸甲酯(PMMA)棒之间的粘结情况,钴铬合金在37℃水中浸泡一个月或在4℃至60℃之间进行60次热循环后,粘结强度均超过150 Kg/cm2。

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验