Nordin Noraini, Kanagesan Samikannu, Zamberi Nur Rizi, Yeap Swee Keong, Abu Nadiah, Tamilselvan Subramani, Hashim Mansor, Alitheen Noorjahan Banu
Department of Cell and Molecular Biology, Faculty of Biotechnology and Biomolecular Sciences, University Putra Malaysia, 43400 Serdang, Selangor, Malaysia.
Materials Synthesis and Characterization Laboratory (MSCL), Institute of Advanced Technology (ITMA), Universiti Putra Malaysia, 43400 Serdang, Selangor, Malaysia.
IET Nanobiotechnol. 2017 Apr;11(3):343-348. doi: 10.1049/iet-nbt.2016.0007.
In this study, nanocrystalline magnesium zinc ferrite nanoparticles were successfully prepared by a simple sol-gel method using copper nitrate and ferric nitrate as raw materials. The calcined samples were characterised by differential thermal analysis/thermogravimetric analysis, Fourier transform infrared spectroscopy and X-ray diffraction. Transmission electron microscopy revealed that the average particle size of the calcined sample was in a range of 17-41 nm with an average of 29 nm and has spherical size. A cytotoxicity test was performed on human breast cancer cells (MDA MB-231) and (MCF-7) at various concentrations starting from (0 µg/ml) to (800 µg/ml). The sample possessed a mild toxic effect toward MDA MB-231 and MCF-7 after being examined with MTT (3-[4, 5-dimethylthiazol-2-yl]-2, 5 diphenyltetrazolium bromide) assay for up to 72 h of incubation. Higher reduction of cells viability was observed as the concentration of sample was increased in MDA MB-231 cell line than in MCF-7. Therefore, further cytotoxicity tests were performed on MDA MB-231 cell line.
在本研究中,以硝酸铜和硝酸铁为原料,通过简单的溶胶-凝胶法成功制备了纳米晶镁锌铁氧体纳米颗粒。采用差示热分析/热重分析、傅里叶变换红外光谱和X射线衍射对煅烧后的样品进行了表征。透射电子显微镜显示,煅烧后样品的平均粒径在17-41nm范围内,平均粒径为29nm,且呈球形。对人乳腺癌细胞(MDA MB-231)和(MCF-7)进行了细胞毒性测试,浓度范围从(0μg/ml)到(800μg/ml)。在用MTT(3-[4,5-二甲基噻唑-2-基]-2,5-二苯基四氮唑溴盐)法检测并孵育长达72小时后,该样品对MDA MB-231和MCF-7具有轻微的毒性作用。在MDA MB-231细胞系中,随着样品浓度的增加,细胞活力的降低比在MCF-7细胞系中更为明显。因此,对MDA MB-231细胞系进行了进一步的细胞毒性测试。