Hirano S, Hirasawa T
Shika Rikogaku Zasshi. 1979 Jan;20(49):40-3.
To research the possibility of a new dental Au base alloy, Au-Ni alloys were examined. Comospitions were 82.5% Au-17.5% Ni alloy, 77% Au-23% Ni alloy and 70% Au-30% Ni alloy. Mechanical properties of these alloys were equal to those of hardened Au added Pt alloy or type IV Au alloy. And these alloys have shown no tarnish and corrosion in 0.1% NaS solution, 0.05% HC1 solution or 1% Lactic acid solution after 21 days. Especially 77% Au-23% Ni alloy was the best among them.
为研究一种新型牙科金基合金的可能性,对金镍合金进行了研究。其成分分别为82.5%金 - 17.5%镍合金、77%金 - 23%镍合金和70%金 - 30%镍合金。这些合金的机械性能与添加铂的硬化金合金或IV型金合金相当。并且这些合金在0.1%硫化钠溶液、0.05%盐酸溶液或1%乳酸溶液中浸泡21天后未出现变色和腐蚀现象。其中,77%金 - 23%镍合金表现最佳。