Wang Xiaodong, Wu Guangming, Zhou Bin, Shen Jun
Shanghai Key Laboratory of Special Artificial Microstructure Materials and Technology, Pohl Institute of Solid State Physics, Tongji University, Siping Road 1239, Shanghai 200092, China.
Materials (Basel). 2012 Dec 24;6(1):76-84. doi: 10.3390/ma6010076.
TiO₂-SiO₂ binary coatings were deposited by a sol-gel dip-coating method using tetrabutyl titanate and tetraethyl orthosilicate as precursors. The structure and chemical composition of the coatings annealed at different temperatures were analyzed by Raman spectroscopy and Fourier Transform Infrared (FTIR) spectroscopy. The refractive indices of the coatings were calculated from the measured transmittance and reflectance spectra. An increase in refractive index with the high temperature thermal annealing process was observed. The Raman and FTIR results indicate that the refractive index variation is due to changes in the removal of the organic component, phase separation and the crystal structure of the binary coatings.
采用溶胶-凝胶浸涂法,以钛酸四丁酯和正硅酸四乙酯为前驱体,制备了TiO₂-SiO₂二元涂层。通过拉曼光谱和傅里叶变换红外(FTIR)光谱分析了在不同温度下退火的涂层的结构和化学成分。根据测得的透过率和反射率光谱计算涂层的折射率。观察到高温热退火过程中折射率增加。拉曼和FTIR结果表明,折射率变化是由于二元涂层中有机成分的去除、相分离和晶体结构的变化所致。