Davies J P, Jasty M, O'Connor D O, Burke D W, Harrigan T P, Harris W H
Orthopaedic Research Laboratories, Massachusetts General Hospital, Boston, MA 02114.
J Bone Joint Surg Br. 1989 Jan;71(1):39-42. doi: 10.1302/0301-620X.71B1.2915001.
We have tested the porosity and fatigue life of five commonly used bone cements: Simplex P, LVC, Zimmer regular, CMW and Palacos R. Tests were conducted with and without centrifugation and with the monomer at room temperature and, except for LVC, at 0 degrees C. We found that the fatigue life of different specimens varied by a factor of nearly 100. It did not depend on porosity alone, but was more influenced by the basic composition of the cement. Simplex P when mixed with monomer at 0 degrees C and centrifuged for 60 seconds had the highest fatigue life and was still sufficiently liquid to use easily.
Simplex P、LVC、Zimmer常规型、CMW和Palacos R。测试分别在离心和未离心的情况下进行,单体温度为室温,除LVC外,还有0摄氏度的情况。我们发现不同样本的疲劳寿命相差近100倍。它并非仅取决于孔隙率,而是更多地受骨水泥基本成分的影响。Simplex P在0摄氏度与单体混合并离心60秒时具有最高的疲劳寿命,且仍具有足够的流动性以便于使用。