Suppr超能文献

抗生素浸渍对 Simplex P 和 Palacos R 丙烯酸骨水泥疲劳寿命的影响,有无离心处理。

Influence of antibiotic impregnation on the fatigue life of Simplex P and Palacos R acrylic bone cements, with and without centrifugation.

作者信息

Davies J P, O'Connor D O, Burke D W, Harris W H

机构信息

Orthopaedic Biomechanics Laboratory, Massachusetts General Hospital, Boston.

出版信息

J Biomed Mater Res. 1989 Apr;23(4):379-97. doi: 10.1002/jbm.820230402.

Abstract

The fatigue properties of Simplex P and Palacos R bone cements were compared to their antibiotic impregnated counterparts AKZ* and Palacos R with gentamycin. The effect of porosity reduction by centrifugation of all four cement types was also assessed. Fifteen specimens of each cement type were prepared according to manufacturer's instructions and 15 additional specimens of each cement type were prepared by mixing the powder with chilled monomer (0 degrees C) and then centrifuging the cement immediately after mixing. Fifteen fully reversed tension-compression fatigue tests were performed at 15 MPa in stress control for each cement preparation in vitro while simulating the in vivo state (37 degrees C and 100% humidity). The number of cycles to failure were recorded. There was no significant difference in the fatigue life of Palacos R and Simplex P when both cements were prepared in the standard fashion. The addition of 1/2 g of gentamycin to Palacos R did not significantly alter its fatigue properties. The addition of 0.5 g of erythromycin and 0.24 g of colistin did not decrease the fatigue life of Simplex P. Centrifugation significantly improved the fatigue properties of Simplex P and AKZ. The fatigue lives of Palacos R and Palacos R with gentamycin were not improved by centrifugation. The fatigue life of centrifuged Simplex P was significantly greater than the fatigue life of Palacos R and of Palacos R with gentamycin, whether the Palacos R based cements were centrifuged or not.

摘要

将Simplex P和Palacos R骨水泥的疲劳性能与其含抗生素的对应产品AKZ*和含庆大霉素的Palacos R进行了比较。还评估了对所有四种骨水泥类型进行离心以降低孔隙率的效果。每种骨水泥类型按照制造商说明制备15个样本,每种骨水泥类型还额外制备15个样本,方法是将粉末与冷却的单体(0摄氏度)混合,然后在混合后立即对骨水泥进行离心。在体外模拟体内状态(37摄氏度和100%湿度)下,对每种骨水泥制剂在应力控制为15 MPa的条件下进行15次完全反向拉伸-压缩疲劳试验。记录失效时的循环次数。当两种骨水泥均以标准方式制备时,Palacos R和Simplex P的疲劳寿命没有显著差异。向Palacos R中添加1/2 g庆大霉素并未显著改变其疲劳性能。添加0.5 g红霉素和0.24 g黏菌素并未降低Simplex P的疲劳寿命。离心显著改善了Simplex P和AKZ的疲劳性能。离心并未改善Palacos R和含庆大霉素的Palacos R的疲劳寿命。无论基于Palacos R的骨水泥是否经过离心,离心后的Simplex P的疲劳寿命均显著长于Palacos R和含庆大霉素的Palacos R的疲劳寿命。