Moosavi Horieh, Hakimi Narjes
Associate Professor, Dental Materials Research Center, Department of Operative Dentistry, Mashhad Dental School, Mashhad University of Medical Sciences, Mashhad, Iran.
Post graduate student, Dental Materials Research Center, Department of Operative Dentistry, Mashhad Dental School, Mashhad University of Medical Sciences, Mashhad, Iran.
J Clin Exp Dent. 2017 Dec 1;9(12):e1390-e1396. doi: 10.4317/jced.54044. eCollection 2017 Dec.
This study investigated the effect of post bleaching treatments to the change of enamel elastic modulus and microhardness after dental bleaching .
Fifty bovine incisor slab were randomly assigned into five groups (n=10). The samples were bleached for three times; 20 minutes each time, by 40% hydrogen peroxide. Next it was applied fractional CO2 laser for two minutes, Nano- hydroxy apatite (N-HA) and MI-paste for 7 days and 2 minutes per day. The sound enamel and bleached teeth without post treatment remained as control groups. The elastic modulus and microhardness were measured at three times; 24 hours, 1 and 2 months. Data were statistically analyzed by two-way analysis of variance with 95% confidence level.
Different methods of enamel treatment caused a significant increase in elastic modulus compared to bleached group (<0.05). Modulus was significantly increased in 1 and 2 months (<0/001: bleach, = 0/015: laser, = 0/008: NHA, =0/010: MI paste) but there were no significantly difference between 1 and 2 months (>0.05). There was any significance difference for hardness among treated and control groups, but hardness increased significantly by increasing storage time (<0.05).
The use of the protective tested agents can be useful in clinical practice to reduce negative changes of enamel surface after whitening procedures. Bleaching enamel, CO2 laser, MI pastes, Nano-hydroxy apatite, Microhardness, Elastic modulus.
本研究调查了牙齿漂白后进行的后续处理对牙釉质弹性模量和显微硬度变化的影响。
将50个牛切牙切片随机分为五组(n = 10)。样本用40%过氧化氢漂白三次,每次20分钟。接下来分别应用分次二氧化碳激光照射两分钟、纳米羟基磷灰石(N - HA)和MI糊剂处理7天,每天两分钟。未进行后续处理的正常牙釉质和漂白牙齿作为对照组。分别在24小时、1个月和2个月这三个时间点测量弹性模量和显微硬度。数据采用95%置信水平的双向方差分析进行统计学分析。
与漂白组相比,不同的牙釉质处理方法导致弹性模量显著增加(<0.05)。在1个月和2个月时模量显著增加(<0.001:漂白组,= 0.015:激光组,= 0.008:NHA组,= 0.010:MI糊剂组),但1个月和2个月之间无显著差异(>0.05)。处理组和对照组之间的硬度无显著差异,但硬度随储存时间的增加而显著增加(<0.05)。
在临床实践中,使用经测试的保护剂有助于减少美白程序后牙釉质表面的负面变化。牙釉质漂白、二氧化碳激光、MI糊剂、纳米羟基磷灰石、显微硬度、弹性模量。