Abstract

OBJECTIVE

This study evaluated the effect of shortened application time on long-term bond strength with universal adhesives.

METHODS AND MATERIALS

Three universal adhesives were used: Clearfil Universal Bond (CU, Kuraray Noritake Dental Inc, Tokyo, Japan), Scotchbond Universal Adhesive (SB, 3M ESPE, St Paul, MN, USA) or G-Premio Bond (GP, GC Corp, Tokyo, Japan). Sixty molars were cut to expose midcoronal dentin and prepared with a regular diamond bur. Each adhesive was applied either according to the manufacturer's instruction or with shortened time. Specimens were stored in distilled water at 37°C for 24 hours and then cut into resin-dentin sticks. Microtensile bond strength (μTBS) was tested after either 24 hours or 1 year of water storage. Data were analyzed by the three-way ANOVA and Duncan tests ( α=0.05). Fracture modes were analyzed under a scanning electron microscope (SEM). One dentin stick per group was selected after fracture mode analysis and further observed using transmission electron microscopy (TEM). Six additional dentin discs were prepared and conditioned with each adhesive under the different application time to observe the adhesive-smear layer interaction by SEM.

RESULTS

Shortened application time affected the μTBS ( p<0.001) while storage time did not affect bond strength ( p=0.187). A significant effect of shortened application time on μTBS was observed in the CU at 1 year and in the GP at both storage times.

CONCLUSIONS

One-year storage time had no effect on the μTBS of universal adhesives to bur-cut dentin. The performance of universal adhesives can be compromised when applied using a shortened application time.

摘要

目的

本研究评估缩短涂抹时间对通用型粘结剂长期粘结强度的影响。

方法与材料

使用三种通用型粘结剂:Clearfil通用粘结剂(CU,可乐丽诺瑞特牙科公司,东京,日本)、Scotchbond通用粘结剂(SB,3M ESPE公司,圣保罗,明尼苏达州,美国)或G-Premio Bond(GP,GC公司,东京,日本)。将60颗磨牙切割以暴露牙冠中部牙本质,并用常规金刚砂车针进行预备。每种粘结剂均按照制造商说明或缩短时间进行涂抹。标本在37°C蒸馏水中储存24小时,然后切割成树脂-牙本质棒。在水储存24小时或1年后测试微拉伸粘结强度(μTBS)。数据通过三因素方差分析和邓肯检验进行分析(α=0.05)。在扫描电子显微镜(SEM)下分析断裂模式。在断裂模式分析后,每组选择一根牙本质棒,并使用透射电子显微镜(TEM)进一步观察。另外制备6个牙本质片,并用每种粘结剂在不同涂抹时间进行处理,以通过SEM观察粘结剂-玷污层相互作用。

结果

缩短涂抹时间影响μTBS(p<0.001),而储存时间不影响粘结强度(p=0.187)。在1年时的CU组以及两个储存时间的GP组中,观察到缩短涂抹时间对μTBS有显著影响。

结论

一年的储存时间对通用型粘结剂与车针切割牙本质的μTBS没有影响。当使用缩短的涂抹时间应用通用型粘结剂时,其性能可能会受到影响。