We present a model to estimate the osteolysis-free life of total hip arthroplasty, depending on linear wear rate and femoral head size. An estimate of the radiologic osteolysis threshold was calculated, which was based on volumetric wear. The osteolysis-free life of the cup was estimated from the quotient of the osteolysis threshold and volumetric wear rate, which was calculated from the linear wear rate. The impact of the direction of linear wear was determined by sensitivity analysis. From our review, we calculated a weighted mean polyethylene volume of approximately 670 mm as osteolysis threshold. Osteolysis-free life of less than 20 years was estimated for linear wear rates of 50 µm/year for head sizes of 32 mm or more, or for linear wear rates of 100 µm/year for any head size. For head sizes of 36 and 40 mm with a linear wear rate of 50 µm/year, the osteolysis-free period is estimated to be only 14.10 and 11.42 years, respectively. Sensitivity analysis showed reasonably robust results. With the aim of osteolysis-free life of more than 20 years, our study presents a viable model to determine maximum possible head size for articulations. Osteolysis-free period for 36 and 40 mm head sizes are far too low for conventional polyethylenes. As the threshold wear volume for highly crosslinked polyethylene is, as of yet, unknown, more research is warranted before our model can be generalized to XLPE.
我们提出了一种模型,用于根据线性磨损率和股骨头尺寸来估计全髋关节置换术的无骨溶解使用寿命。计算了基于体积磨损的放射学骨溶解阈值估计值。髋臼的无骨溶解使用寿命是根据骨溶解阈值与由线性磨损率计算得出的体积磨损率的商来估计的。通过敏感性分析确定了线性磨损方向的影响。通过我们的综述,我们计算出约670立方毫米的加权平均聚乙烯体积作为骨溶解阈值。对于32毫米及以上的股骨头尺寸,线性磨损率为50微米/年,或对于任何股骨头尺寸,线性磨损率为100微米/年,估计无骨溶解使用寿命小于20年。对于36毫米和40毫米的股骨头尺寸,线性磨损率为50微米/年,无骨溶解期估计分别仅为14.10年和11.42年。敏感性分析显示结果相当稳健。为了实现超过20年的无骨溶解使用寿命,我们的研究提出了一个可行的模型来确定关节的最大可能股骨头尺寸。对于传统聚乙烯,36毫米和40毫米股骨头尺寸的无骨溶解期过低。由于高度交联聚乙烯的阈值磨损体积目前尚不清楚,在我们的模型能够推广到交联聚乙烯之前,还需要更多的研究。