Clin Oral Investig. 2019 Aug;23(8):3275-3285. doi: 10.1007/s00784-018-2749-7. Epub 2018 Nov 28.
The aim of this study was to assess the effects of three different fluoride-releasing agents on preventing white spot lesions that occur during treatment with full coverage rapid maxillary expanders.
A total of 48 patients with transverse maxillary deficiency were randomly assigned to four equal groups. A fluoride-containing agent was applied to teeth before cementation of the full coverage acrylic-bonded rapid maxillary expanders in the three experimental groups (gel, varnish, and sealent in groups 1, 2, and 3, respectively), while the control group received no agent application. Quantitative light-induced fluorescence (QLF) images of the patients were obtained before cementation and after decementation of the appliances. Four parameters (ΔF, ΔF, A, and ΔR) were evaluated on maxillary ten anterior teeth.
In the fluoride gel group, upper central and lateral incisors, right first and left second premolars showed significant decreases in fluorescence levels indicating demineralization. Right central and left lateral incisors showed significant white spot lesion formation in the fluoride varnish group. Right and left central incisors and left first premolar were the teeth that mineral loss was observed in the sealent group, while all of the teeth except canines and first premolars showed significant demineralization in the control group.
Multifluorid varnish and Proseal sealant were effective on preventing demineralization and should be applied to teeth clinically before appliance cementation.
Demineralization is a major problem during orthodontic treatment. The application of effective fluoride-releasing agents could prevent this major iatrogenic complication.
本研究旨在评估三种不同的氟释放剂在预防全冠快速扩弓器治疗过程中发生的白斑病的效果。
共 48 例横向上颌骨发育不足的患者被随机分为四组。在三组实验(1 组凝胶、2 组涂料、3 组密封剂)中,在全冠丙烯酸粘结快速扩弓器粘固前,将含氟剂应用于牙齿,而对照组则未应用任何含氟剂。在粘固前和器械拆除后,对患者的定量光诱导荧光(QLF)图像进行了获取。对上颌前牙的 10 颗牙齿评估了四个参数(ΔF、ΔF、A 和 ΔR)。
在氟凝胶组中,上颌中切牙和侧切牙、右侧第一和左侧第二前磨牙的荧光水平显著降低,表明脱矿。氟涂料组中右侧中切牙和左侧侧切牙出现明显的白斑病形成。在密封剂组中,右侧和左侧中切牙以及左侧第一前磨牙出现矿质损失,而对照组中除尖牙和第一前磨牙外,所有牙齿均出现明显脱矿。
多氟涂料和 Proseal 密封剂在预防脱矿方面有效,应在临床应用器械前将其应用于牙齿。
脱矿是正畸治疗中的一个主要问题。应用有效的氟释放剂可以预防这种主要的医源性并发症。