Department of Operative Dentistry and Endodontics, Mahidol University.
Dent Mater J. 2019 Mar 31;38(2):287-294. doi: 10.4012/dmj.2017-333. Epub 2019 Feb 1.
This study determined the micro-shear bond strength (µSBS) of two self-etching adhesives to dentin surface after smear layer removal with a novel ultrasonic brushing method. Ninety-five dentin discs were ground flat with diamond burs and divided into 5 groups; no treatment (control), brushing with a custom-made brush for 10 and 30 s without and with ultrasonic application. The smear layer thickness was evaluated using SEM. The 24 h µSBS of Clearfil SE Bond (CSE) and Clearfil Tri S Bond (CTS) to these dentin surfaces were evaluated. Smear layer thickness decreased significantly from control, brushing without, and brushing with ultrasonic groups, respectively. The µSBS of CSE were higher than CTS in all groups. The µSBS were improved with ultrasonic brushing for 30 s for both adhesives. Ultrasonic brushing is the effective method in mechanical smear layer removal which can improve bond strength of self-etching adhesives to ground dentin.
本研究旨在确定在使用新型超声刷洗法去除玷污层后,两种自酸蚀黏合剂对牙本质表面的微剪切黏结强度(µSBS)。将 95 个牙本质圆盘用金刚石磨具磨平,并分为 5 组;不处理(对照)、用定制刷刷洗 10 秒和 30 秒、不施加和施加超声。使用 SEM 评估玷污层厚度。评估 Clearfil SE Bond(CSE)和 Clearfil Tri S Bond(CTS)在这些牙本质表面的 24 小时µSBS。与对照、无超声刷洗和有超声刷洗组相比,玷污层厚度显著降低。在所有组中,CSE 的µSBS 均高于 CTS。两种黏合剂均经过 30 秒超声刷洗,µSBS 得到提高。超声刷洗是一种有效的机械去除玷污层的方法,可以提高自酸蚀黏合剂对研磨牙本质的黏结强度。