Suppr超能文献

采用电化学沉淀法在等离子体电解氧化处理的Ti-6Al-4V合金上制备功能元素涂层

Functional Elements Coatings on the Plasma Electrolytic Oxidation-Treated Ti-6Al-4V Alloy by Electrochemical Precipitation Method.

作者信息

Kim Seung-Pyo, Choe Han-Cheol

机构信息

Department of Dental Materials and Research Center of Nano-Interface Activation for Biomaterials, College of Dentistry, Chosun University, Gwangju, 61452, Korea.

出版信息

J Nanosci Nanotechnol. 2019 Jul 1;19(7):4344-4349. doi: 10.1166/jnn.2019.16278.

Abstract

In this study, functional elements coatings on the plasma electrolytic oxidation (PEO)-treated Ti-6Al-4V alloy by electrochemical precipitation method were investigated. Ti-6Al-4V ELI disks were used as specimens for PEO and HA coating. The applied voltage and time were selected to be 280 V and 3 minutes for PEO treatment, respectively. The electrochemical precipitation on the Ti-6Al-4V alloy was carried out using cyclic voltammetry with cycle of 3, 5, 10, and 20 from -1.5 V to 0 V (vs. SCE electrode) in electrolyte containing Ca, P, Mg, Mn, Sr, Zn, and Si ions by cyclic voltammetry after PEO treatment. The morphology changes of the coatings on the PEO treated Ti-6Al-4V alloy surface were observed using FE-SEM and EDS. PEO surface has a uniformly distributed circular shape and a porous surface and the deposition of low cycles in electrolyte containing Mg, Mn, Sr, Zn, and Si-HA coated surfaces show uniform circular and granular structures. The precipitates of Mg, Mn, Sr, Zn, and Si-HA on the PEO treated surface showed a large number of circular particles as the number of deposition cycles increases with a mixture of rod-shaped particles and petal-shaped particles around pores. The precipitate nucleates around the pore and grows rapidly as the cycles increase.

摘要

在本研究中,对通过电化学沉淀法在等离子体电解氧化(PEO)处理的Ti-6Al-4V合金上制备的功能元素涂层进行了研究。采用Ti-6Al-4V ELI圆盘作为PEO和HA涂层的试样。PEO处理的施加电压和时间分别选择为280 V和3分钟。在含有Ca、P、Mg、Mn、Sr、Zn和Si离子的电解液中,通过循环伏安法在-1.5 V至0 V(相对于SCE电极)范围内进行3、5、10和20个循环,对PEO处理后的Ti-6Al-4V合金进行电化学沉淀。使用场发射扫描电子显微镜(FE-SEM)和能谱仪(EDS)观察PEO处理的Ti-6Al-4V合金表面涂层的形貌变化。PEO表面具有均匀分布的圆形形状和多孔表面,在含有Mg、Mn、Sr、Zn和Si的HA涂层表面进行低循环沉积时,呈现出均匀的圆形和颗粒状结构。随着沉积循环次数的增加,PEO处理表面上Mg、Mn、Sr、Zn和Si-HA的沉淀物显示出大量圆形颗粒,在孔隙周围有棒状颗粒和花瓣状颗粒的混合物。沉淀物在孔隙周围成核,并随着循环次数的增加而迅速生长。