Suppr超能文献

外膜磷脂酶A(A1)在氧化石墨烯基FeO纳米颗粒中的重组表达及其用于菜籽油脱胶的固定化

Recombinant Expression of Outer Membrane Phospholipase A (A1) in and Immobilization With Graphene Oxide-Based FeO Nanoparticles for Rapeseed Oil Degumming.

作者信息

Yang Peizhou, Jiang Suwei, Wu Yun, Hou Zhigang, Zheng Zhi, Cao Lili, Du Mingrui, Jiang Shaotong

机构信息

Anhui Key Laboratory of Intensive Processing of Agricultural Products, College of Food and Biological Engineering, Hefei University of Technology, Hefei, China.

出版信息

Front Microbiol. 2019 Feb 21;10:334. doi: 10.3389/fmicb.2019.00334. eCollection 2019.

Abstract

Enzymatic degumming is an effective approach to produce nutritional, safe, and healthy refined oil. However, the high cost and low efficiency of phospholipase limit the application of enzymatic degumming. In this study, an 879 bp outer membrane phospholipase A (A1) (OM-PLA1) gene encoding 292 amino acid residues was isolated from the genome of . The recombinant OM-PLA1 profile of appropriately 33 KDa was expressed by the engineered GS115. The OM-PLA1 activity was 21.2 U/mL with the induction of 1 mM methanol for 72 h. The expression efficiencies of OM-PLA1 were 0.29 U/mL/h and 1.06 U/mL/OD600. A complex of magnetic graphene oxide (MGO) and OM-PLA1 (MGO-OM-PLA1) was prepared by immobilizing OM-PLA1 with graphene oxide-based FeO nanoparticles by cross-linking with glutaraldehyde. The content of phosphorus decreased to 5.1 mg/kg rapeseed oil from 55.6 mg/kg rapeseed oil with 0.02% MGO-OM-PLA1 (w/w) at 50°C for 4 h. MGO-OM-PLA1 retained 51.7% of the initial activity after 13 times of continuous recycling for the enzymatic degumming of rapeseed oil. This study provided an effective approach for the enzymatic degumming of crude vegetable oil by developing a novel phospholipase and improving the degumming technology.

摘要

酶法脱胶是生产营养、安全且健康的精炼油的有效方法。然而,磷脂酶的高成本和低效率限制了酶法脱胶的应用。在本研究中,从……的基因组中分离出一个编码292个氨基酸残基的879 bp外膜磷脂酶A(A1)(OM-PLA1)基因。工程菌GS115表达出了约33 KDa的重组OM-PLA1。在1 mM甲醇诱导72 h后,OM-PLA1活性为21.2 U/mL。OM-PLA1的表达效率分别为0.29 U/mL/h和1.06 U/mL/OD600。通过用基于氧化石墨烯的FeO纳米颗粒与戊二醛交联固定OM-PLA1,制备了磁性氧化石墨烯(MGO)与OM-PLA1的复合物(MGO-OM-PLA1)。在50℃下用0.02%(w/w)的MGO-OM-PLA1处理4 h后,菜籽油中的磷含量从55.6 mg/kg降至5.1 mg/kg。MGO-OM-PLA1在连续13次用于菜籽油酶法脱胶后仍保留了51.7%的初始活性。本研究通过开发新型磷脂酶和改进脱胶技术,为粗植物油的酶法脱胶提供了一种有效方法。

https://cdn.ncbi.nlm.nih.gov/pmc/blobs/19da/6393389/db8ce3a66226/fmicb-10-00334-g001.jpg

文献检索

告别复杂PubMed语法,用中文像聊天一样搜索,搜遍4000万医学文献。AI智能推荐,让科研检索更轻松。

立即免费搜索

文件翻译

保留排版,准确专业,支持PDF/Word/PPT等文件格式,支持 12+语言互译。

免费翻译文档

深度研究

AI帮你快速写综述,25分钟生成高质量综述,智能提取关键信息,辅助科研写作。

立即免费体验