Lopez Chelsi, Park Shiwha, Edwards Seth, Vong Selina, Hou Shujie, Lee Minyoung, Sauerland Hunter, Lee Jung-Jae, Jeong Kyung Jae
Department of Chemistry, University of Colorado Denver, Denver, CO 80204.
Department of Chemical Engineering, University of New Hampshire, Durham, NH 03824.
ACS Biomater Sci Eng. 2019 Mar 11;5(3):1195-1199. doi: 10.1021/acsbiomaterials.8b01404. Epub 2019 Jan 4.
Corneal melting is an uncontrolled, excessive degradation of cellular and extracellular components of the cornea. This potential cause of corneal blindness is caused by excessive expression of zinc-dependent matrix metalloproteinases (MMPs) and has no satisfying cure as of now. Herein, we introduce a novel therapeutic hydrogel which can be made into a contact lens to slow down the progression of corneal melting by deactivating MMPs. The hydrogel backbone is comprised of poly(2-hydroxyetyl methacrylate) (pHEMA), a main material for commercial contact lenses, and dipicolylamine (DPA) which has high affinity and selectivity towards zinc ion. Due to the high affinity towards zinc ions, the DPA-conjugated pHEMA (pDPA-HEMA) hydrogel selectively removes zinc ions from a physiological buffer and deactivates MMP-1, MMP-2 and MMP-9 within 2 hours. pDPA-HEMA hydrogel also effectively prevents degradation of porcine corneas by collagenase A, a zinc-dependent protease, whereas the corneas completely degrades within 15 hours when incubated with pHEMA hydrogel. The presence of pDPA-HEMA hydrogel does not affect the viability of keratocytes and corneal epithelial cells. Unlike the conventional MMP inhibitors (MMPi), the pDPA-HEMA hydrogel minimizes the risk of serious non-specific side effects, and provides a method to slow down the progression of corneal melting and other related ocular diseases.
角膜溶解是角膜细胞和细胞外成分不受控制的过度降解。这种导致角膜失明的潜在原因是锌依赖性基质金属蛋白酶(MMPs)的过度表达,目前尚无令人满意的治疗方法。在此,我们介绍一种新型治疗性水凝胶,它可以制成隐形眼镜,通过使MMPs失活来减缓角膜溶解的进展。水凝胶主链由聚甲基丙烯酸羟乙酯(pHEMA,商业隐形眼镜的主要材料)和对锌离子具有高亲和力和选择性的二吡啶甲胺(DPA)组成。由于对锌离子具有高亲和力,DPA共轭的pHEMA(pDPA-HEMA)水凝胶可从生理缓冲液中选择性去除锌离子,并在2小时内使MMP-1、MMP-2和MMP-9失活。pDPA-HEMA水凝胶还能有效防止锌依赖性蛋白酶胶原酶A对猪角膜的降解,而与pHEMA水凝胶孵育时,角膜在15小时内会完全降解。pDPA-HEMA水凝胶的存在不影响角膜细胞和角膜上皮细胞的活力。与传统的MMP抑制剂(MMPi)不同,pDPA-HEMA水凝胶将严重非特异性副作用的风险降至最低,并提供了一种减缓角膜溶解和其他相关眼部疾病进展的方法。