Suppr超能文献

具有疏水表面的亲水性折射多焦点人工晶状体的表面下钙化:病例系列

Subsurface calcification of hydrophilic refractive multifocal intraocular lenses with a hydrophobic surface: A case series.

作者信息

Bang Seung Pil, Moon Kun, Lee Jong-Ho, Jun Jong Hwa, Joo Choun-Ki

机构信息

Department of Ophthalmology, Keimyung University School of Medicine, Daegu.

Department of Biomedical Engineering, University of Rochester, Rochester, NY, United States.

出版信息

Medicine (Baltimore). 2019 Dec;98(50):e18379. doi: 10.1097/MD.0000000000018379.

Abstract

RATIONALE

Opacification of monofocal intraocular lenses (IOLs) of various designs and materials has been reported. Hydrophilic acrylic IOLs are more prone to opacification than hydrophobic IOLs, but IOL surface modification by hydrophobic materials may improve biocompatibility, and few opacifications of such monofocal lenses have been reported to date. However, here we describe the characteristics of opacification of hydrophilic refractive multifocal IOLs with a hydrophobic surface modification in a cluster of patients who underwent uneventful cataract surgery.

PATIENT CONCERNS

In this retrospective observational case series, the medical records of 7 patients in whom opacification of the IOL was identified after implantation of LS-313 MF30 (Lentis M plus, Oculentis), from November 2017 to May 2019, were reviewed.

DIAGNOSIS

All patients had undergone bilateral implantation of LS-313 MF30 IOLs. Ten eyes of 7 patients showed significant opacification at a mean 49.1 ± 10.2 months postoperatively.

INTERVENTIONS

The IOLs of 4 cases were explanted.

OUTCOMES

All of the opacified cases had received LS-313 MF30 IOLs from February 2014 to August 2014 and experienced decreased visual acuity after 44.6 ± 10.5 months. The explanted IOLs of 4 cases were evaluated by scanning electron microscopy (SEM), energy-dispersive X-ray spectroscopy (EDX), Alizarin-red, and von Kossa staining. These explanted IOLs showed fine and evenly distributed, whitish deposits on the entire IOL, particularly below the surface. Although the constituent of the deposits was identified as calcium by Alizarin-red and von Kossa stain, SEM, and EDX analysis showed no surface deposits of calcium. Paraffin-embedded sections of the IOLs were prepared, and calcium deposition was confirmed by EDX analysis at the subsurface region of the IOL.

LESSENS

Significant opacification of these hydrophilic refractive multifocal IOLs with hydrophobic surface modification was found to be due to abnormal calcification of the subsurface of the IOL. Clinicians must be aware of the opacification of this IOL design, despite surface modification. In particular, it should be noted that there is a high likelihood that the patient may experience vision-related symptoms even with moderate opacity and that opacification may lead to a burdensome IOL exchange.

摘要

原理

已有报道称各种设计和材料的单焦点人工晶状体(IOL)会出现混浊。亲水性丙烯酸酯IOL比疏水性IOL更容易发生混浊,但用疏水性材料对IOL表面进行改性可能会提高生物相容性,且迄今为止,此类单焦点晶状体很少有混浊的报道。然而,在此我们描述了一组白内障手术顺利的患者中,具有疏水性表面改性的亲水性折射多焦点IOL的混浊特征。

患者情况

在这个回顾性观察病例系列中,我们回顾了2017年11月至2019年5月期间7例在植入LS-313 MF30(Lentis M plus,Oculentis)后被发现IOL混浊的患者的病历。

诊断

所有患者均接受了双侧LS-313 MF30 IOL植入。7例患者的10只眼在术后平均49.1±10.2个月出现明显混浊。

干预措施

4例患者的IOL被取出。

结果

所有混浊病例均在2014年2月至2014年8月期间接受了LS-313 MF30 IOL,在44.6±10.5个月后视力下降。对4例患者取出的IOL进行了扫描电子显微镜(SEM)、能量色散X射线光谱(EDX)、茜素红和冯·科萨染色评估。这些取出的IOL在整个IOL上显示出细小且分布均匀的白色沉积物,尤其是在表面下方。尽管通过茜素红和冯·科萨染色确定沉积物的成分是钙,但SEM和EDX分析显示IOL表面没有钙沉积物。制备了IOL的石蜡包埋切片,并通过EDX分析在IOL的亚表面区域证实了钙沉积。

经验教训

发现这些具有疏水性表面改性的亲水性折射多焦点IOL的明显混浊是由于IOL亚表面的异常钙化。尽管进行了表面改性,临床医生仍必须意识到这种IOL设计可能出现混浊。特别是,应该注意的是,即使混浊程度适中,患者也很可能会出现与视力相关的症状,并且混浊可能导致繁重的IOL置换。

https://cdn.ncbi.nlm.nih.gov/pmc/blobs/a38b/6922436/5b0c316116ca/medi-98-e18379-g001.jpg

文献检索

告别复杂PubMed语法,用中文像聊天一样搜索,搜遍4000万医学文献。AI智能推荐,让科研检索更轻松。

立即免费搜索

文件翻译

保留排版,准确专业,支持PDF/Word/PPT等文件格式,支持 12+语言互译。

免费翻译文档

深度研究

AI帮你快速写综述,25分钟生成高质量综述,智能提取关键信息,辅助科研写作。

立即免费体验