Schwarz Ivana, Kovačević Stana, Vitlov Ivana
Department of Textile Design and Management, Faculty of Textile Technology, University of Zagreb, Prilaz baruna Filipovića 28a, 10000 Zagreb, Croatia.
School of Applied Arts and Design, Perivoj Vladimira Nazora 3/3, 23000 Zadar, Croatia.
Polymers (Basel). 2020 Dec 27;13(1):73. doi: 10.3390/polym13010073.
The investigation of influential parameters of the starching process on mechanical properties of yarns intended for multifunctional woven fabrics for thermal protective clothing was performed on four different yarn samples starched on an innovative starching machine, adapted to industrial starching conditions. The starching was conducted with two different processes with different starch mass concentrations: the standard starching process and a newer starching process (with yarn prewetting). Based on the results obtained, it can be concluded that starching positively affects all the properties of tested samples and that the increase of starch mass concentration is not accompanied by the improvement of those yarn properties. Synthetic polymer fibers that achieve satisfactory yarn strength need to be starched with lower starch mass concentrations in order to retain the breaking properties and to be protected from abrasion and static electricity, which occurs during the weaving process. The yarn prewetting starching process shows significantly better results than the standard starching process, especially for aramid yarns, where abrasion resistance increased from 42 to 135%. Therefore, we can conclude that the goal of starching such yarns is aimed at increasing the wear resistance. Linear regressions and correlations between the values of breaking properties and abrasion resistance obtained by the testing and their values that were estimated by the analysis show a high correlation coefficient.
在一台适应工业上浆条件的创新型浆纱机上,对用于热防护服多功能机织面料的纱线进行上浆处理,针对四种不同的纱线样品,研究了上浆过程的影响参数对纱线机械性能的影响。上浆采用两种不同工艺,具有不同的淀粉质量浓度:标准上浆工艺和一种较新的上浆工艺(纱线预湿)。根据所得结果可以得出结论,上浆对测试样品的所有性能都有积极影响,并且淀粉质量浓度的增加并未伴随着纱线性能的改善。为了保持断裂性能并防止在织造过程中产生的磨损和静电,达到令人满意纱线强度的合成聚合物纤维需要用较低的淀粉质量浓度进行上浆。纱线预湿上浆工艺的效果明显优于标准上浆工艺,特别是对于芳纶纱线,其耐磨性从42%提高到了135%。因此,我们可以得出结论,对这类纱线上浆的目的是提高耐磨性。通过测试获得的断裂性能值和耐磨性值与通过分析估计的值之间的线性回归和相关性显示出较高的相关系数。