Dent Mater J. 2021 Sep 30;40(5):1257-1263. doi: 10.4012/dmj.2020-142. Epub 2021 Jun 30.
The bonding performance of a surface pre-reacted glass ionomer (S-PRG) filler-containing self-adhesive flowable resin composites to enamel and dentin were evaluated using a tensile bond test with thermal cycling. Also, the quantities of various ions released from the materials were measured using ICP atomic emission spectrometry and a fluoride ion electrode. The initial bond strengths of the materials were approximately 6 MPa, and decreased after thermal cycling. The S-PRG filler-containing self-adhesive flowable resin composites materials exhibited much higher ion release compared with the commercial self-adhesive flowable resin composite possibly due to different acidic monomers contained. It was suggested that the S-PRG filler containing self-adhesive flowable resin composites should be limited as a lining material or to restore small cavities in non-stress bearing areas.
采用热循环拉伸结合试验评价了一种表面预反应玻璃离子(S-PRG)填料型自粘接流动树脂复合材料对牙釉质和牙本质的粘结性能,并采用 ICP 原子发射光谱仪和氟离子电极测量了材料释放的各种离子的量。材料的初始粘结强度约为 6MPa,热循环后降低。与商用自粘接流动树脂复合材料相比,S-PRG 填料型自粘接流动树脂复合材料的离子释放量更高,这可能是由于其中含有不同的酸性单体。因此建议将含有 S-PRG 填料的自粘接流动树脂复合材料限制用于衬里材料或在非承重区域修复小的龋洞。