Hart D E
Contact Lens Research Foundation, Jericho, NY 11753.
J Am Optom Assoc. 1987 Dec;58(12):962-74.
SEM was used to visualize tear-film/hydrogel polymer surface interactions. Lenses were preserved by fixation including a quaternary ammonium complex to aid in mucin preservation. In less than 2 weeks of continuous wear the anterior surface was completely coated, yet the coating was absent from the posterior lens surface. Tear-film break-up over the deposited lens surface, combined with degradation and deformation at the polymer surface boundary, as well as entrapment of moieties within the polymer matrix, all occurred. These are the likely culprits which can contribute to adverse reactions as well as cause light scatter and diminished vision. Lenses removed directly from the eyes of patients suffering with different forms of conjunctivitis were obtained. Bacterial and viral conjunctivitis can induce a microbially contaminated as well as a heavily deformed and deposited lens. Viable and intact microbes were not typically observed in the mucoprotein layer of hydrogel contact lenses.
扫描电子显微镜用于观察泪膜/水凝胶聚合物表面的相互作用。通过包含季铵络合物的固定方法来保存镜片,以帮助保存黏蛋白。在连续佩戴不到2周的时间里,镜片前表面被完全覆盖,但后表面没有涂层。沉积镜片表面的泪膜破裂,聚合物表面边界处的降解和变形,以及聚合物基质内部分子的截留都发生了。这些可能是导致不良反应、引起光散射和视力下降的罪魁祸首。获取了直接从患有不同形式结膜炎的患者眼中取出的镜片。细菌性和病毒性结膜炎可导致镜片被微生物污染,以及严重变形和沉积。在水凝胶隐形眼镜的黏蛋白层中通常未观察到存活且完整的微生物。