Abstract

It was the intention of the study to evaluate the etching effects of several self-etching primers on unground enamel and their relevance for shear bond strength testing. Seven self-etching primers (Clearfil SE, Futurabond NR, M-Bond, One Coat, Optibond, Transbond SEP+, Xeno III) and a conventional 35% phosphoric gel acid were applied to bovine incisors according to the manufacturer's instructions. All specimens were analyzed by electron microscopy. A visual four-step grading was used for the characterization of the macroscopic (5000×) and microscopic (20,000×) etching patterns. In addition, shear bond strength for all the products was tested with an Instron 3344 after 1000 thermocycles between 5 °C and 55 °C. Statistical analysis was carried out using Kruskal-Wallis with Dunn's post-test and Pearson's correlation coefficient. Very strong etching patterns with well-defined prisms were found for the conventional etching, Transbond SEP+, and to a lesser degree, for Xeno III. Clearfil SE and Futurabond NR revealed moderate etching patterns, and M-Bond, One Coat, and Optibond revealed very weak etching patterns. The bond strength correlated well with the etching patterns. The highest shear strength was obtained with conventional etching and Transbond SEP+, followed by Clearfil SE. Moderate shear bond strengths were found for Xeno III, Futurabond NR, One Coat, and M-Bond, and the lowest were found with Optibond.

摘要

本研究旨在评估几种自酸蚀底漆对未打磨牙釉质的蚀刻效果及其与剪切粘结强度测试的相关性。按照制造商的说明,将七种自酸蚀底漆(Clearfil SE、Futurabond NR、M-Bond、One Coat、Optibond、Transbond SEP+、Xeno III)和一种传统的35%磷酸凝胶酸应用于牛的切牙。所有标本均通过电子显微镜进行分析。采用视觉四步分级法对宏观(5000倍)和微观(20000倍)蚀刻模式进行表征。此外,在5℃至55℃之间进行1000次热循环后,使用Instron 3344对所有产品的剪切粘结强度进行测试。使用Kruskal-Wallis检验和Dunn事后检验以及Pearson相关系数进行统计分析。对于传统蚀刻、Transbond SEP+以及程度稍低的Xeno III,发现具有清晰界定棱柱的非常强的蚀刻模式。Clearfil SE和Futurabond NR显示出中等蚀刻模式,而M-Bond、One Coat和Optibond显示出非常弱的蚀刻模式。粘结强度与蚀刻模式相关性良好。传统蚀刻和Transbond SEP+获得了最高的剪切强度,其次是Clearfil SE。Xeno III、Futurabond NR、One Coat和M-Bond的剪切粘结强度中等,Optibond的最低。

https://cdn.ncbi.nlm.nih.gov/pmc/blobs/250e/8621149/3ab64689a344/dentistry-09-00138-g001.jpg

文献检索

告别复杂PubMed语法,用中文像聊天一样搜索,搜遍4000万医学文献。AI智能推荐,让科研检索更轻松。

立即免费搜索

文件翻译

保留排版,准确专业,支持PDF/Word/PPT等文件格式,支持 12+语言互译。

免费翻译文档

深度研究

AI帮你快速写综述,25分钟生成高质量综述,智能提取关键信息,辅助科研写作。

立即免费体验