The aim of this study was to evaluate the micro-shear bond strength (µSBS) of one and two steps self-etch adhesive systems after enamel bleaching with photo-activated bleaching systems of different hydrogen peroxide (HP) concentration. Occlusal enamel of forty intact human molars were flattened and assigned into four groups. GI Unbleached, GII, GIII, and GIV were bleached with Pyrenees (3.5% HP), GC TiON (20% HP), and Hi-Lite (35% HP) respectively. Enamel treatment with one and two steps self-etch adhesives (Clearfil S3 Bond- S3, and Clearfil SE Bond-SE) then micro-tubes were fixed on enamel and filled with AP-X composite (n=5). Bond was tested with the universal testing machine. Data were analyzed using two-way ANOVA and Tukey's tests at 5 % level of significance. The µSBS was significantly different between adhesives (F=154.46; p<0.05) and bleaching systems (F=77.33; p<0.05) with significant interaction. Specimens bonded with S3 shows a significantly lower μSBS than those bonded with SE (p<0.05) in all groups. For both adhesives the bleached groups demonstrate lower µSBS than unbleached except specimens bleached with Pyrenees and bonded with SE (p>0.05). A significant difference was observed between groups of the bleaching systems (p<0.05). Different peroxide concentrations photo-activated bleaching systems adversely affect μSBS of one and two steps self-etch adhesives. Low concentration system (Pyrenees) does not influence the bond strength of two steps adhesive.
本研究旨在评估光激活漂白系统不同浓度过氧化氢(HP)对釉质漂白后一步法和两步法自酸蚀粘接剂的微剪切粘接强度(µSBS)。将四十颗完整的人磨牙的咬合面釉质磨平,分为四组。GI 未漂白组、GII、GIII 和 GIV 分别用 Pyrenees(3.5% HP)、GC TiON(20% HP)和 Hi-Lite(35% HP)漂白。用一步法和两步法自酸蚀粘接剂(Clearfil S3 Bond-S3 和 Clearfil SE Bond-SE)处理釉质,然后将微管固定在釉质上并用 AP-X 复合材料填充(n=5)。用万能试验机进行粘接测试。数据采用双因素方差分析和 Tukey 检验,显著性水平为 5%。粘接剂(F=154.46;p<0.05)和漂白系统(F=77.33;p<0.05)之间的 µSBS 有显著差异,存在显著的交互作用。与 SE 相比,S3 粘结的样本 µSBS 明显较低(p<0.05),所有组均如此。对于两种粘接剂,除了用 Pyrenees 漂白并用 SE 粘结的样本外(p>0.05),漂白组的 µSBS 均低于未漂白组。漂白系统的各组之间存在显著差异(p<0.05)。不同浓度的光激活漂白系统会对一步法和两步法自酸蚀粘接剂的 µSBS 产生不利影响。低浓度系统(Pyrenees)不会影响两步法粘接剂的粘结强度。