Vukelja Josipa, Klarić Sever Eva, Sever Ivan, Jukić Krmek Silvana, Tarle Zrinka
Department of Endodontics and Restorative Dentistry, School of Dental Medicine, University of Zagreb, 10000 Zagreb, Croatia.
Thinktourism, 10000 Zagreb, Croatia.
Materials (Basel). 2021 Dec 12;14(24):7664. doi: 10.3390/ma14247664.
The aim of this in vitro study was to assess the effect of two different adhesive application methods on shear dentin bond strength (ISO 29022) using three various adhesive systems. A mid-coronal section of 77 intact third human molars with fully developed apices was made to create flat bonding substrates. The materials used in the study were Excite F (Ivoclar Vivadent), Prime&Bond Universal (Dentsply Sirona) and G-Premio Bond (GC). The application of each adhesion system was performed in two different ways. In the first group, the bonding agent was light cured immediately after the application (conventional method), while in the second group the adhesive and composite were cured concurrently ("co-curing" method). A total of 180 specimens were prepared (3 adhesives × 2 method of application × 30 specimens per experimental group), stored at 37 °C in distilled water and fractured in shear mode after 1 week. Statistical analysis was performed using ANOVA and Weibull statistics. The highest bond strength was obtained for Prime&Bond conventional (21.7 MPa), whilst the lowest bond strength was observed when co-curing was used (particularly, Excite F 12.2 MPa). The results showed a significant difference between conventional and co-curing methods in all materials. According to reliability analysis, the co-curing method diminished bond reliability. Different application techniques exhibit different bond strengths to dentin.
本体外研究的目的是使用三种不同的粘结系统,评估两种不同的粘结剂应用方法对牙本质剪切粘结强度(ISO 29022)的影响。对77颗根尖完全发育的完整人类第三磨牙进行牙冠中部切片,以制作平坦的粘结基底。本研究中使用的材料为Excite F(义获嘉伟瓦登特公司)、Prime&Bond Universal(登士柏西诺德公司)和G-Premio Bond(GC公司)。每种粘结系统的应用以两种不同方式进行。在第一组中,粘结剂在应用后立即光固化(传统方法),而在第二组中,粘结剂和复合材料同时固化(“共固化”方法)。总共制备了180个样本(3种粘结剂×2种应用方法×每组30个样本),在37℃的蒸馏水中储存1周后,以剪切模式断裂。使用方差分析和威布尔统计进行统计分析。Prime&Bond传统方法获得的粘结强度最高(21.7MPa),而使用共固化时观察到的粘结强度最低(特别是Excite F为12.2MPa)。结果表明,所有材料的传统方法和共固化方法之间存在显著差异。根据可靠性分析,共固化方法降低了粘结可靠性。不同的应用技术对牙本质表现出不同的粘结强度。