J Adhes Dent. 2022 Mar 24;24:77-86. doi: 10.3290/j.jad.b2838105.
To evaluate the clinical performance of direct composite restorations using nanohybrid and nanofill composite materials in anterior teeth in patients with amelogenesis imperfecta (AI).
The study included 15 patients with AI aged 14-30 years. During the study, the patients received anterior direct composite laminate veneer restorations using either a nanohybrid (Clearfil Majesty ES-2 and Clearfil Universal Bond, Kuraray Noritake) or a nanofill resin composite (Filtek Ultimate Universal Restorative and Single Bond Universal Adhesive, 3M Oral Care). The restorations were evaluated according to the modified USPHS criteria at baseline and at 1-, 2-, 3- and 4-year follow-up periods.
The cumulative success rate of anterior restorations was 80.5% for nanohybrid and 92.5% for nanofill composite after 4 years. Eight restorations with nanohybrid and three restorations with nanofill resin composites failed. Ten restorations failed due to fracture; the fracture rate was 12.3%. Statistically significant differences were found between nanohybrid and nanofill composites regarding marginal discoloration and surface texture after 3 years. Furthermore, statistically significant differences were observed with respect to color match after 4 years.
The use of a nanohybrid or nanofill composite for anterior direct restorations in patients with AI was observed to be satisfactory, based on the rate of ideal and clinically acceptable restorations. The primary reason for restoration failure was fracture. The failure rate of nanohybrid composite restorations was higher than with nanofill composite restorations with respect to survival and marginal adaptation criteria.
评估在釉质发育不全患者的前牙中使用纳米复合树脂和纳米复合树脂材料进行直接复合修复的临床性能。
本研究纳入了 15 名年龄在 14-30 岁的釉质发育不全患者。在研究过程中,这些患者接受了前牙直接复合层压贴面修复,使用的材料分别是纳米复合树脂(Clearfil Majesty ES-2 和 Clearfil Universal Bond,Kuraray Noritake)或纳米复合树脂(Filtek Ultimate Universal 修复体和Single Bond Universal 黏结剂,3M 口腔护理)。在基线、1、2、3 和 4 年随访时,根据改良美国公共卫生协会(USPHS)标准评估修复体。
在 4 年的随访中,纳米复合树脂的前牙修复体总成功率为 80.5%,纳米复合树脂的总成功率为 92.5%。纳米复合树脂有 8 个修复体失败,纳米复合树脂有 3 个修复体失败。10 个修复体因折断而失败,折断率为 12.3%。在 3 年后,纳米复合树脂和纳米复合树脂的边缘变色和表面质地有统计学差异。此外,在 4 年后,颜色匹配方面也存在统计学差异。
在釉质发育不全患者的前牙直接修复中,使用纳米复合树脂或纳米复合树脂材料的修复效果是令人满意的,这体现在理想和临床可接受修复体的比例上。修复失败的主要原因是折断。在生存和边缘适应性标准方面,纳米复合树脂修复体的失败率高于纳米复合树脂修复体。