Suppr超能文献

直接树脂复合修复体治疗上颌牙折裂和关闭间隙:7 年回顾性生存分析及影响因素。

Direct resin composite restorations for fractured maxillary teeth and diastema closure: A 7 years retrospective evaluation of survival and influencing factors.

机构信息

Department of Restorative Dentistry and Periodontology, University of Pécs, Pécs, Hungary.

Department of Restorative Dentistry and Periodontology, University of Pécs, Pécs, Hungary.

出版信息

Dent Mater. 2017 Apr;33(4):467-476. doi: 10.1016/j.dental.2017.02.001. Epub 2017 Feb 28.

Abstract

OBJECTIVES

This retrospective study evaluated the survival rate of anterior direct resin based composite (RBC) build-ups in vital teeth made of microhybrid and nanofill RBC materials and the influence of bruxism, beverage consumption and smoking on the long-term performance of restorations.

METHODS

Patients receiving anterior restoration between 2006 and 2011, with the diagnosis of fracture or diastema, were selected. A total of 65 adult patients (mean age: 25.2) with 163 restorations (78 Filtek Supreme XT and 85 Enamel Plus HFO) were evaluated using the USPHS criteria. Data were analyzed with Fisher's Exact Test, Extended Cox-regression analysis and Kaplan-Meier method.

RESULTS

Mean observation period was 7.2 (±1.4) years and the mean annual failure rate for this period was 1.43%. The reasons of failures included restoration fracture and color mismatch. Nanofill restorations had significantly higher rate of color mismatch (p=0.002), microhybrids more frequently failed in fracture of restoration (p=0.034). The overall difference in potential hazard of using Enamel Plus HFO or Filtek Supreme XT was not significant (p=0.704). Chipping or fracture of the restoration was more frequent in the first year after placement (p=0.036), while beverage consumption was significantly correlated with discoloration of the restorations (p=0.005).

SIGNIFICANCE

The application of direct RBC restorations provides an excellent treatment option for fractured teeth and for closing diastemas. The overall survival rate was 88.34% up to 10 years. Microhybrid and nanofill RBC restorations showed similar survival rates, however nanofills discolored at a higher rate, meanwhile chipping of the restoration occurred frequently with microhybrids.

摘要

目的

本回顾性研究评估了微混合和纳米填充型直接复合树脂在前牙活髓牙修复中的存活率,并探讨了磨牙症、饮料摄入和吸烟对修复体长期性能的影响。

方法

选择 2006 年至 2011 年间接受前牙修复的患者,诊断为牙折或牙间隙。共评估了 65 名成年患者(平均年龄 25.2 岁)的 163 个修复体(78 个 Filtek Supreme XT 和 85 个 Enamel Plus HFO),使用 USPHS 标准进行评估。采用 Fisher 确切检验、扩展 Cox 回归分析和 Kaplan-Meier 法进行数据分析。

结果

平均观察期为 7.2(±1.4)年,在此期间的年平均失败率为 1.43%。失败的原因包括修复体折裂和颜色不匹配。纳米填充修复体的颜色不匹配发生率显著较高(p=0.002),微混合修复体更频繁地出现修复体折裂(p=0.034)。使用 Enamel Plus HFO 或 Filtek Supreme XT 的潜在危险总体差异无统计学意义(p=0.704)。修复体的崩瓷或折裂更常见于放置后的第一年(p=0.036),而饮料摄入与修复体变色显著相关(p=0.005)。

意义

直接复合树脂修复为牙折和关闭牙间隙提供了一种极好的治疗选择。10 年内的总体存活率为 88.34%。微混合和纳米填充型直接复合树脂修复体的存活率相似,但纳米填充体颜色变色率较高,而微混合体修复体的崩瓷发生率较高。