Suppr超能文献

由废弃大理石和矿渣粉制成的硫磺混凝土:100%可回收且无水的混凝土。

Sulfur concrete made with waste marble and slag powders: 100% recycled and waterless concrete.

作者信息

Rasheed Muhammad Faisal, Rahim Abdur, Irfan-Ul-Hassan Muhammad, Ali Babar, Ali Nazam

机构信息

Research Scholar, Department of Transportation Engineering and Management, University of Engineering & Technology, Lahore, Pakistan.

Assistant Professor, Department of Civil Engineering, University of Engineering & Technology, Lahore, Pakistan.

出版信息

Environ Sci Pollut Res Int. 2022 Sep;29(43):65655-65669. doi: 10.1007/s11356-022-20456-y. Epub 2022 Apr 30.

Abstract

In this research, the mechanical properties and durability of sulfur concrete with two different waste aggregates were evaluated. The waste aggregates included ground granulated blast-furnace slag and waste marble powder. The properties of sulfur concrete were also compared with those of the conventional binder concretes (i.e., Portland cement concrete and sulfate-resistant cement concrete). The durability parameters included measuring water absorption capacity and resistance to different harsh chemical environments (5% HCl solution, 5 Molar NaOH solution, and 16% NaCl solution). It was found that sulfur concrete made with slag as aggregate exhibited the maximum strength, i.e., about 2 times higher than that of Portland cement concrete and sulfate-resistant cement concrete. Sulfur concrete made with slag and marble waste powder showed superior mechanical performance compared to that made with river sand. Thus, sulfur binder develops more favorable properties with eco-friendly fillers than it develops with natural sand. In harsh chloride and acidic environment, sulfur concrete with slag powder exhibited about 90-95% lesser mass loss than Portland cement concrete.

摘要

在本研究中,对含有两种不同废弃骨料的硫磺混凝土的力学性能和耐久性进行了评估。废弃骨料包括粒化高炉矿渣和废弃大理石粉。还将硫磺混凝土的性能与传统胶凝材料混凝土(即硅酸盐水泥混凝土和抗硫酸盐水泥混凝土)的性能进行了比较。耐久性参数包括测量吸水能力以及对不同恶劣化学环境(5%盐酸溶液、5摩尔氢氧化钠溶液和16%氯化钠溶液)的抗性。结果发现,以矿渣为骨料制成的硫磺混凝土表现出最大强度,即比硅酸盐水泥混凝土和抗硫酸盐水泥混凝土高出约两倍。与用河砂制成的硫磺混凝土相比,用矿渣和大理石废粉制成的硫磺混凝土表现出更优异的力学性能。因此,与天然砂相比,硫磺胶凝材料与环保填料形成的性能更优。在恶劣的氯化物和酸性环境中,含矿渣粉的硫磺混凝土的质量损失比硅酸盐水泥混凝土少约90 - 95%。