Maso Patrícia Canova, Souza Matheus Albino, Borba Márcia, Goedel Fábio, Farina Ana Paula, Cecchin Doglas, Maso Daniele Canova, Dogenski Letícia Copatti, Corazza Pedro Henrique, Palhano Huriel Scartazzini, Rauber Bárbara Facco, De Carli João Paulo
School of Dentistry, University of Passo Fundo, Passo Fundo, RS, Brazil.
School of Engineering, University of Passo Fundo, Passo Fundo, RS, Brazil.
Photodiagnosis Photodyn Ther. 2022 Dec;40:103180. doi: 10.1016/j.pdpdt.2022.103180. Epub 2022 Oct 30.
To evaluate the influence of photodynamic therapy (PDT), different final irrigants, and ultrasonic activation (US) on the bond strength of glass fiber posts (GFP) to root dentin.
One hundred twenty bovine roots were divided into 12 groups according to PDT application, the type of final endodontic irrigant, and US. The samples were divided into 12 groups (n = 10): G1-DW(distilled water); G2-DW+US; G3-17% EDTA; G4-17% EDTA+US; G5-17% GA (glycolic acid); G6-17% GA+US; G7-PDT+DW; G8-PDT+DW+US; G9-PDT+17% EDTA; G10-PDT+17% EDTA+US; G11-PDT+17% GA; G12-PDT+17% GA+US. After cementing the glass fiber posts with resin cement, roots were sectioned into 2-mm-thick slices. One slice from the cervical third and another from the middle third were used for the push out test (PO), and the other two for the diametral compression test (DC). Thus, 10 samples were obtained per third for each mechanical test (n = 10). Kruskal-Wallis and Student-Newman-Keuls tests were used to analyze PO and DC data, and Pearson's correlation test was used to verify the relationship between the variables. Failure patterns were analyzed with chi-square test.
Significant differences were found in the PO test among the experimental groups (p < 0.001; power=1.00). PDT improved bond strength when using EDTA. PDT and US increased bond strength when using GA. Favorable failure patterns occurred more frequently in Group GA+US. There was no correlation between data obtained with PO and DC tests (r = 0.112; p = 0.729).
PDT provided the highest bond strength values of GFP to root dentin when associated with GA and US or when associated only with EDTA.
评估光动力疗法(PDT)、不同的终末冲洗液以及超声激活(US)对玻璃纤维桩(GFP)与牙根牙本质粘结强度的影响。
根据PDT应用、终末根管冲洗液类型和US,将120颗牛牙根分为12组。样本分为12组(n = 10):G1 - 蒸馏水(DW);G2 - DW + US;G3 - 17%乙二胺四乙酸(EDTA);G4 - 17% EDTA + US;G5 - 17%乙醇酸(GA);G6 - 17% GA + US;G7 - PDT + DW;G8 - PDT + DW + US;G9 - PDT + 17% EDTA;G10 - PDT + 17% EDTA + US;G11 - PDT + 17% GA;G12 - PDT + 17% GA + US。用树脂水门汀粘结玻璃纤维桩后,将牙根切成2毫米厚的薄片。从颈段三分之一处取一片,中段三分之一处取另一片用于推出试验(PO),另外两片用于径向压缩试验(DC)。因此,每个力学试验每三分之一段获得10个样本(n = 10)。采用Kruskal - Wallis和Student - Newman - Keuls检验分析PO和DC数据,采用Pearson相关检验验证变量之间的关系。用卡方检验分析失败模式。
实验组间在PO试验中发现显著差异(p < 0.001;检验效能 = 1.00)。使用EDTA时,PDT提高了粘结强度。使用GA时,PDT和US增加了粘结强度。在GA + US组中,有利的失败模式更频繁出现。PO试验和DC试验获得的数据之间无相关性(r = 0.112;p = 0.729)。
当与GA和US联合使用或仅与EDTA联合使用时,PDT能使GFP与牙根牙本质获得最高的粘结强度值。