Prim Dent J. 2023 Mar;12(1):88-95. doi: 10.1177/20501684231154323.
A range of materials for single-tooth computer-aided design and computer-aided manufacturing (CAD-CAM) restorations have been introduced that may affect CAM accuracy. This study aimed to review articles evaluating marginal and internal fit of lithium disilicate (LD) and zirconia (Z) crowns fabricated by CAD-CAM systems using intraoral optical scanners (IOS).
Under the guidelines of Preferred Reporting Items for Systematic Reviews and Meta-analysis (PRISMA), a systematic review was performed along with an electronic article search in the Medline/Pubmed database. The articles were limited to those in the English language that were published within the past ten years.
The initial search resulted in 50 articles and of those, a total of 18 articles were selected for full-text review following abstract evaluation. Eight articles that did not meet the inclusion criteria were excluded and the remaining ten articles, which provided internal and marginal gap values, were used in this review. For LD crowns, marginal gap values ranged between 45µm and 190.2µm. For Z crowns, the values varied between 39µm and 126.4µm. For LD crowns, the internal gap values were between 57.8µm and 475.4µm, and for Z crowns, the values were between 79µm and 205.8µm.
The outcome of this review suggests that clinically acceptable marginal and internal fit can be attained with LD and Z all-ceramic CAD-CAM crowns using digital impressions. Additionally, it has been found that LD and Z ceramics provide similar marginal gap values, but LD material provides better internal fit than Z.
已经引入了一系列用于单颗牙齿计算机辅助设计和计算机辅助制造(CAD-CAM)修复的材料,这些材料可能会影响 CAM 精度。本研究旨在回顾评估使用口腔内光学扫描仪(IOS)制造的 CAD-CAM 系统制作的锂硅玻璃陶瓷(LD)和氧化锆(Z)冠的边缘和内部适合性的文章。
根据系统评价和荟萃分析的首选报告项目(PRISMA)指南,在 Medline/Pubmed 数据库中进行了系统评价和电子文章搜索。文章仅限于过去十年内以英文发表的文章。
最初的搜索产生了 50 篇文章,其中有 18 篇文章经过摘要评估后被选中进行全文审查。排除了 8 篇不符合纳入标准的文章,其余 10 篇提供内部和边缘间隙值的文章被用于本综述。对于 LD 冠,边缘间隙值在 45μm 和 190.2μm 之间。对于 Z 冠,值在 39μm 和 126.4μm 之间。对于 LD 冠,内部间隙值在 57.8μm 和 475.4μm 之间,对于 Z 冠,值在 79μm 和 205.8μm 之间。
本综述的结果表明,使用数字印模可以获得临床可接受的 LD 和 Z 全陶瓷 CAD-CAM 冠的边缘和内部适合性。此外,发现 LD 和 Z 陶瓷提供相似的边缘间隙值,但 LD 材料的内部拟合优于 Z。