Orabi Kassab Bashi Mhd Amer, Bshara Nada, Alzoubi Hasan
Department of Pediatric Dentistry, Damascus University, Damascus, SYR.
Cureus. 2023 Feb 15;15(2):e35005. doi: 10.7759/cureus.35005. eCollection 2023 Feb.
Background and purpose The aesthetic requirements for the restoration of the primary anterior teeth of both the child and his parents increased recently, especially with the presence of materials with good mechanical properties capable of giving a good aesthetic shape. However, the challenge remains in the possibility of applying these materials to primary teeth, where the child's cooperation and ability to keep their mouth open during the completion of the restoration is an important challenge for the dentist. Therefore, this study aimed to evaluate the bonding of self-adhesive composite by studying the microleakage in primary canines. Materials and methods The studied sample consisted of 60 extracted primary canines that were divided into three equal groups (n=20) according to the type of restoration: group 1 (experimental) - self-adhesive composite alone, group 2 (experimental) - self-adhesive composite with selective enamel etching, and group 3 (control) - conventional composite with the self-etching bond and selective enamel etching. A Class V cavity was prepared at the cementoenamel junction, 2 mm deep and 1 mm in diameter. In this way, the gingival wall is dentine, while the incisal wall is enamel-dentine. Restorations were placed according to the group to which the tooth belongs. After that, all teeth were subjected to 500 cycles of thermocycling. Then, a methylene blue dye microleakage test was performed, and longitudinal sections of the teeth were made and studied under x20 magnification using a stereo microscope. Results In the gingival wall, the scores of microleakage in the conventional composite group after selective etching were lower than those of the self-adhesive composite groups, with a statistically significant difference. While in the incisal wall, there were no statistically significant differences in the frequencies of the scores of microleakage between the three groups. Conclusions Within the limitations of this study, the conventional composite bonded better to enamel and dentine than self-adhesive composite resin applied alone or after selective enamel etching. The bonding of the self-adhesive composite was lower than that of the conventional composite, and it is not recommended to use it in Class V restorations of primary anterior teeth.
背景与目的 近期,儿童及其家长对乳前牙修复的美学要求有所提高,尤其是出现了具有良好机械性能、能赋予良好美学外形的材料。然而,将这些材料应用于乳牙仍面临挑战,因为在修复过程中,患儿的配合度以及保持口腔张开的能力对牙医来说是一项重要挑战。因此,本研究旨在通过研究乳尖牙的微渗漏情况来评估自黏结复合树脂的黏结性能。
材料与方法 研究样本包括60颗拔除的乳尖牙,根据修复类型分为三个相等的组(n = 20):第1组(实验组)——仅使用自黏结复合树脂;第2组(实验组)——自黏结复合树脂结合选择性釉质酸蚀;第3组(对照组)——传统复合树脂结合自酸蚀黏结剂和选择性釉质酸蚀。在牙骨质釉质界制备一个V类洞,深2 mm,直径1 mm。这样,龈壁为牙本质,而切壁为釉质 - 牙本质。根据牙齿所属组别进行修复。之后,所有牙齿进行500次热循环。然后,进行亚甲蓝染料微渗漏试验,并制作牙齿纵剖面,使用体视显微镜在20倍放大倍数下进行观察。
结果 在龈壁,选择性酸蚀后传统复合树脂组的微渗漏评分低于自黏结复合树脂组,差异具有统计学意义。而在切壁,三组微渗漏评分的频率差异无统计学意义。
结论 在本研究的局限性范围内,传统复合树脂与釉质和牙本质的黏结效果优于单独使用或选择性釉质酸蚀后使用的自黏结复合树脂。自黏结复合树脂的黏结性能低于传统复合树脂,不建议将其用于乳前牙的V类修复。