Suppr超能文献

CO激光切割后木材横截面表面不规则性的评估。

Evaluation of the Surface Irregularities of the Cross-Section of the Wood after CO Laser Cutting.

作者信息

Adamčík Lukáš, Igaz Rastislav, Štefančin Lukáš, Kubovský Ivan, Kminiak Richard

机构信息

Faculty of Wood Sciences and Technology, Technical University in Zvolen, T.G. Masaryka 24, 96001 Zvolen, Slovakia.

出版信息

Materials (Basel). 2023 Nov 15;16(22):7175. doi: 10.3390/ma16227175.

Abstract

The present paper deals with the analysis of cross-section surface irregularities after CO laser cutting. The surface irregularities of beech ( L.), oak (), and spruce ( L.) wood were quantified by primary profile parameters using a digital microscope. The arithmetic mean height (Pa), used as the basic parameter, was supplemented by amplitude parameters (Pv, Pp, Pz) and the Psm parameter, through which the shape of the irregularity was specified in more detail. A statistically significant change was demonstrated when changing the values of the feed speed and the power of the CO laser. The results of this article confirm that the surface irregularities increased with an increasing laser power and decreasing feed rate. The scanned topographic images also provide a more detailed explanation of the measured P-parameters and point out the risks associated with the evaluation of the cross-section with the primary profile.

摘要

本文论述了CO激光切割后横截面表面不规则性的分析。使用数字显微镜通过主要轮廓参数对山毛榉(L.)、橡木()和云杉(L.)木材的表面不规则性进行了量化。作为基本参数的算术平均高度(Pa),由幅度参数(Pv、Pp、Pz)和Psm参数进行补充,通过这些参数可以更详细地确定不规则性的形状。当改变CO激光的进给速度和功率值时,显示出具有统计学意义的变化。本文的结果证实,表面不规则性随着激光功率的增加和进给速度的降低而增加。扫描的地形图像还对测量的P参数提供了更详细的解释,并指出了使用主要轮廓评估横截面所涉及的风险。

https://cdn.ncbi.nlm.nih.gov/pmc/blobs/d757/10673011/89df661e3359/materials-16-07175-g001.jpg

文献检索

告别复杂PubMed语法,用中文像聊天一样搜索,搜遍4000万医学文献。AI智能推荐,让科研检索更轻松。

立即免费搜索

文件翻译

保留排版,准确专业,支持PDF/Word/PPT等文件格式,支持 12+语言互译。

免费翻译文档

深度研究

AI帮你快速写综述,25分钟生成高质量综述,智能提取关键信息,辅助科研写作。

立即免费体验