Pan Peng, Hu Cheng, Liang Ahui, Liu Xueping, Fang Mengqi, Yang Shanlong, Zhang Yadong, Li Mingzhong
National Engineering Laboratory for Modern Silk, College of Textile and Clothing Engineering, Soochow University, Suzhou 215123, China.
Polymers (Basel). 2023 Nov 30;15(23):4581. doi: 10.3390/polym15234581.
The development of a wound dressing with both antibacterial and healing-guiding functions is a major concern in the treatment of open and infected wounds. In this study, poly(hexamethylene biguanide) hydrochloride (PHMB) was loaded into a 3D silk fibroin (SF) scaffold based on electrostatic interactions between PHMB and SF, and PHMB/SF hybrid scaffolds were prepared via freeze-drying. The effects of the PHMB/SF ratio on the antibacterial activity and cytocompatibility of the hybrid scaffold were investigated. The results of an agar disc diffusion test and a bacteriostasis rate examination showed that when the mass ratio of PHMB/SF was greater than 1/100, the scaffold exhibited obvious antibacterial activity against and . L-929 cells were encapsulated in the PHMB/SF scaffolds and cultured in vitro. SEM, laser scanning confocal microscopy, and CCK-8 assay results demonstrated that hybrid scaffolds with a PHMB/SF ratio of less than 2/100 significantly promoted cell adhesion, spreading, and proliferation. In conclusion, a hybrid scaffold with a PHMB/SF ratio of approximately 2/100 not only effectively inhibited bacterial reproduction but also showed good cytocompatibility and is expected to be usable as a functional antibacterial dressing for wound repair.
开发一种兼具抗菌和愈合引导功能的伤口敷料是开放性感染伤口治疗中的一个主要关注点。在本研究中,基于聚六亚甲基双胍盐酸盐(PHMB)与丝素蛋白(SF)之间的静电相互作用,将PHMB负载到三维丝素蛋白支架中,并通过冷冻干燥制备了PHMB/SF混合支架。研究了PHMB/SF比例对混合支架抗菌活性和细胞相容性的影响。琼脂平板扩散试验和抑菌率检测结果表明,当PHMB/SF的质量比大于1/100时,该支架对[具体细菌名称1]和[具体细菌名称2]表现出明显的抗菌活性。将L-929细胞包封在PHMB/SF支架中并进行体外培养。扫描电子显微镜、激光扫描共聚焦显微镜和CCK-8检测结果表明,PHMB/SF比例小于2/100的混合支架能显著促进细胞黏附、铺展和增殖。综上所述,PHMB/SF比例约为2/100的混合支架不仅能有效抑制细菌繁殖,还表现出良好的细胞相容性,有望用作伤口修复的功能性抗菌敷料。